An investigation of material removal rate and surface roughness of squeeze casted A413 alloy on WEDM by multi response optimization using RSM R Soundararajan, A Ramesh, N Mohanraj, N Parthasarathi journal of alloys and compounds 685, 533-545, 2016 | 104 | 2016 |
Correlation between coefficient of friction and surface roughness in dry sliding wear of AISI 316 L (N) stainless steel at elevated temperatures NL Parthasarathi, U Borah, SK Albert Computer Modelling and New Technologies 17 (1), 51-63, 2013 | 49 | 2013 |
Effect of temperature on sliding wear of AISI 316 L (N) stainless steel–Analysis of measured wear and surface roughness of wear tracks NL Parthasarathi, U Borah, SK Albert Materials & Design 51, 676-682, 2013 | 44 | 2013 |
Effect of plasma spraying parameter on wear resistance of NiCrBSiCFe plasma coatings on austenitic stainless steel at elevated temperatures at various loads NL Parthasarathi, M Duraiselvam, U Borah Materials & Design (1980-2015) 36, 141-151, 2012 | 44 | 2012 |
Effect of microstructure on void nucleation and coalescence during forming of three different HSLA steel sheets under different stress conditions R Narayanasamy, NL Parthasarathi, CS Narayanan Materials & Design 30 (4), 1310-1324, 2009 | 44 | 2009 |
High temperature tribological properties of NiCrBSiCFe plasma-sprayed coating on austenitic stainless steel substrate NL Parthasarathi, M Duraiselvam Journal of Alloys and Compounds 505 (2), 824-831, 2010 | 30 | 2010 |
Effect of the tracing speed and span on roughness parameters determined by stylus type equipment MA Davinci, NL Parthasarathi, U Borah, SK Albert Measurement 48, 368-377, 2014 | 28 | 2014 |
Effect of annealing on formability of aluminium grade 19000 R Narayanasamy, NL Parthasarathi Materials & Design 29 (8), 1633-1653, 2008 | 27 | 2008 |
A study on fracture behaviour of three different high strength low alloy steel sheets during formation with different strain ratios R Narayanasamy, NL Parthasarathi, CS Narayanan, T Venugopal, ... Materials & Design 29 (9), 1868-1885, 2008 | 26 | 2008 |
Enhanced visible light photocatalytic activity of P-block elements (C, N and F) doped porous TiO2 coatings on Cp-Ti by micro-arc oxidation S Sridhar, A Viswanathan, K Venkateswarlu, N Rameshbabu, ... Journal of Porous Materials 22, 545-557, 2015 | 20 | 2015 |
Improvement of high temperature wear resistance of AISI 316 ASS through NiCrBSiCFe plasma spray coating NL Parthasarathi, M Duraiselvam Journal of Minerals and Materials Characterization and Engineering 9 (07), 653, 2010 | 16 | 2010 |
Performance analysis in turning of D3 tool steel using silver nanoplatelets as additives under MQL MN Babu, V Anandan, NL Parthasarathi, CV Yildirim, MD Babu, SR Das Journal of the Brazilian Society of Mechanical Sciences and Engineering 44 …, 2022 | 15 | 2022 |
A review on effect of reinforcement and squeeze casting process parameters on mechanical properties of aluminium matrix composites P Saravanakumar, R Soundararajan, PS Deepavasanth, N Parthasarathi International Journal of Innovative Research in Science, Engineering and …, 2016 | 14 | 2016 |
Effect of annealing temperature on void coalescence in 5086 aluminium alloy formed under different stress conditions R Narayanasamy, M Ravi Chandran, C Sathiya Narayanan, ... International Journal of Mechanics and Materials in Design 3 (4), 293-307, 2006 | 13 | 2006 |
Effect of thermal expansion on the high temperature wear resistance of Ni-20% Cr detonation spray coating on IN718 substrate N Purushotham, NL Parthasarathi, PS Babu, G Sivakumar, B Rajasekaran Surface and Coatings Technology 462, 129490, 2023 | 12 | 2023 |
Some analysis on stress and strain limit for necking and fracture during forming of some HSLA steel sheets R Narayanasamy, CS Narayanan, NL Parthasarathi Materials Science and Engineering: A 445, 427-439, 2007 | 11 | 2007 |
Analysis of fracture limit curves and void coalescence in high strength interstitial free steel sheets formed under different stress conditions R Narayanasamy, NL Parthasarathi, R Ravindran, CS Narayanan Journal of materials science 43, 3351-3363, 2008 | 10 | 2008 |
Strain limit of extra galvannealed Interstitial-Free and bake hardened steel sheets under different stress conditions R Narayanasamy, NL Parthasarathi, R Ravindran, CS Narayanan Journal of Iron and Steel Research International 15 (5), 56-60, 2008 | 8 | 2008 |
Sliding wear behaviour of Ni-5% Al coating deposited by detonation spray on IN718 N Purushotham, B Rajasekaran, NL Parthasarathi, K Praveen, ... Materials Today: Proceedings 65, 3741-3747, 2022 | 7 | 2022 |
Influence of stress ratio and contact pressure on fretting fatigue behavior of modified 9Cr-1Mo steel V Shiva, S Goyal, NL Parthasarathi, CR Das, R Kannan, A Nagesha, ... Journal of Materials Engineering and Performance 30, 2822-2831, 2021 | 7 | 2021 |