Heat treatment effect on the microstructure, tensile properties and dry sliding wear behavior of A356–10% B4C cast composites HR Lashgari, S Zangeneh, H Shahmir, M Saghafi, M Emamy Materials & Design 31 (9), 4414-4422, 2010 | 144 | 2010 |
Determination of Johnson–Cook plasticity model parameters for Inconel718 HK Farahani, M Ketabchi, S Zangeneh Journal of Materials Engineering and Performance 26, 5284-5293, 2017 | 71 | 2017 |
Influence of service-induced microstructural changes on the failure of a cobalt-based superalloy first stage nozzle S Zangeneh, H Farhangi Materials & Design 31 (7), 3504-3511, 2010 | 64 | 2010 |
Investigation on microstructure and mechanical properties of Al/Al-Zn-Mg–Cu laminated composite fabricated by accumulative roll bonding (ARB) process SHS Ebrahimi, K Dehghani, J Aghazadeh, MB Ghasemian, S Zangeneh Materials Science and Engineering: A 718, 311-320, 2018 | 62 | 2018 |
Microstructural evolution during isothermal aging and strain-induced transformation followed by isothermal aging in Co-Cr-Mo-C alloy: A comparative study HR Lashgari, S Zangeneh, F Hasanabadi, M Saghafi Materials Science and Engineering: A 527 (16-17), 4082-4091, 2010 | 57 | 2010 |
Fracture failure analysis of AISI 304L stainless steel shaft S Zangeneh, M Ketabchi, A Kalaki Engineering Failure Analysis 36, 155-165, 2014 | 39 | 2014 |
Microstructure and tribological characteristics of aged Co–28Cr–5Mo–0.3 C alloy S Zangeneh, HR Lashgari, A Roshani Materials & Design 37, 292-303, 2012 | 37 | 2012 |
Effect of isothermal aging on the microstructural evolution of Co–Cr–Mo–C alloy S Zangeneh, HR Lashgari, M Saghafi, M Karshenas Materials Science and Engineering: A 527 (24-25), 6494-6500, 2010 | 32 | 2010 |
Assessment of premature failure in a first stage gas turbine nozzle A Malekbarmi, S Zangeneh, A Roshani Engineering Failure Analysis 18 (5), 1262-1271, 2011 | 30 | 2011 |
The effect of Al-5Ti-1B on the microstructure, hardness and tensile properties of a new Zn rich aluminium alloy SZ S.H. Seyed Ebrahimia, J. Aghazadeha, K. Dehghania, M. Emamyb Materials Science and Engineering: A, 2015 | 27 | 2015 |
Determination of residual stress on TIG-treated surface via nanoindentation technique in Co-Cr-Mo-C alloy M Sahami-Nejad, HR Lashgari, S Zangeneh, C Kong Surface and Coatings Technology 380, 125020, 2019 | 23 | 2019 |
Rejuvenation of degraded first stage gas turbine nozzle by heat treatment S Zangeneh, H Farhangi, HR Lashgari Journal of alloys and compounds 497 (1-2), 360-368, 2010 | 22 | 2010 |
Rotary friction welding of additively manufactured 17-4PH stainless steel HR Lashgari, S Li, C Kong, M Asnavandi, S Zangeneh Journal of Manufacturing Processes 64, 1517-1528, 2021 | 21 | 2021 |
The effect of long-term service exposure on the stability of carbides in Co–Cr–Ni–W (X-45) superalloy S Zangeneh, HR Lashgari, M Asnavandi Engineering Failure Analysis 84, 276-286, 2018 | 21 | 2018 |
Fitness for service assessment of a pressure vessel subjected to fire damage in a refinery unit R Bakhtiari, S Zangeneh, MB Fotouh, SM Jamshidi, A Shafeie Engineering Failure Analysis 80, 444-452, 2017 | 21 | 2017 |
Isothermal aging effect on the microstructure and dry sliding wear behavior of Co–28Cr–5Mo–0.3 C alloy HR Lashgari, S Zangeneh, M Ketabchi Journal of materials science 46, 7262-7274, 2011 | 20 | 2011 |
Dry sliding wear characteristics, corrosion behavior, and hot deformation properties of eutectic Al–Si piston alloy containing Ni-rich intermetallic compounds M Mirzaee-Moghadam, HR Lashgari, S Zangeneh, S Rasaee, M Seyfor, ... Materials Chemistry and Physics 279, 125758, 2022 | 16 | 2022 |
Charge storage properties of mixed ternary transition metal ferrites MZnFe oxides (M= Al, Mg, Cu, Fe, Ni) prepared by hydrothermal method M Saghafi, SA Hosseini, S Zangeneh, AH Moghanian, V Salarvand, ... SN Applied Sciences 1, 1-16, 2019 | 15 | 2019 |
Microstructural characterization of TIG surface treating in Co-Cr-Mo-C alloy S Zangeneh, HR Lashgari, HF Lopez, HK Farahani Materials Characterization 132, 223-229, 2017 | 15 | 2017 |
Fitness-for-service assessment and failure analysis of AISI 304 demineralized-water (DM) pipeline weld crack S Zangeneh, HR Lashgari, HR Sharifi Engineering Failure Analysis 107, 104210, 2020 | 14 | 2020 |