A review on non-destructive evaluation of rails: State-of-the-art and future development M Ph Papaelias, C Roberts, CL Davis Proceedings of the Institution of Mechanical Engineers, Part F: Journal of …, 2008 | 418 | 2008 |
Cleavage initiation in the intercritically reheated coarse-grained heat-affected zone: Part I. Fractographic evidence CL Davis, JE King Metallurgical and materials transactions A 25, 563-573, 1994 | 391 | 1994 |
Modeling solid solution strengthening in nickel alloys HA Roth, CL Davis, RC Thomson Metallurgical and Materials Transactions A 28, 1329-1335, 1997 | 322 | 1997 |
Direct visualization of HIV-1-specific cytotoxic T lymphocytes during primary infection JDK Wilson, GS Ogg, RL Allen, C Davis, S Shaunak, J Downie, W Dyer, ... Aids 14 (3), 225-233, 2000 | 232 | 2000 |
The role of deformed rail microstructure on rolling contact fatigue initiation JE Garnham, CL Davis Wear 265 (9-10), 1363-1372, 2008 | 190 | 2008 |
Effect of cooling rate on intercritically reheated microstructure and toughness in high strength low alloy steel CL Davis, JE King Materials Science and technology 9 (1), 8-15, 1993 | 162 | 1993 |
Teaching materials using case studies C Davis, E Wilcock C. Baillie (Series Ed.), The UK Centre for Materials Education. Retrieved …, 2003 | 161 | 2003 |
High-speed inspection of rails using ACFM techniques MP Papaelias, MC Lugg, C Roberts, CL Davis Ndt & E International 42 (4), 328-335, 2009 | 155 | 2009 |
Time efficient auto-focussing algorithms for ultrasonic inspection of dual-layered media using full matrix capture M Weston, P Mudge, C Davis, A Peyton Ndt & E International 47, 43-50, 2012 | 129 | 2012 |
Analysis of the liftoff effect of phase spectra for eddy current sensors W Yin, R Binns, SJ Dickinson, C Davis, AJ Peyton IEEE Transactions on Instrumentation and Measurement 56 (6), 2775-2781, 2007 | 115 | 2007 |
Cleavage initiation in steel: Competition between large grains and large particles A Ghosh, A Ray, D Chakrabarti, CL Davis Materials Science and Engineering: A 561, 126-135, 2013 | 108 | 2013 |
Influential microstructural changes on rolling contact fatigue crack initiation in pearlitic rail steels HC Eden, JE Garnham, CL Davis Materials science and technology 21 (6), 623-629, 2005 | 105 | 2005 |
Charpy-impact-toughness prediction using an “effective” grain size for thermomechanically controlled rolled microalloyed steels D Bhattacharjee, JF Knott, CL Davis Metallurgical and Materials Transactions A 35, 121-130, 2004 | 101 | 2004 |
Modelling of the response of an ACFM sensor to rail and rail wheel RCF cracks GL Nicholson, CL Davis Ndt & E International 46, 107-114, 2012 | 96 | 2012 |
Modelling rail steel microstructure and its effect on crack initiation FJ Franklin, JE Garnham, DI Fletcher, CL Davis, A Kapoor Wear 265 (9-10), 1332-1341, 2008 | 96 | 2008 |
Effect of TiN particles and grain size on the charpy impact transition temperature in steels J Du, M Strangwood, CL Davis Journal of Materials Science & Technology 28 (10), 878-888, 2012 | 95 | 2012 |
Very early stage rolling contact fatigue crack growth in pearlitic rail steels JE Garnham, CL Davis Wear 271 (1-2), 100-112, 2011 | 90 | 2011 |
Measurement of permeability and ferrite/austenite phase fraction using a multi-frequency electromagnetic sensor W Yin, XJ Hao, AJ Peyton, M Strangwood, CL Davis NDT & e International 42 (1), 64-68, 2009 | 86 | 2009 |
Effect of TiN particles and microstructure on fracture toughness in simulated heat-affected zones of a structural steel LP Zhang, CL Davis, M Strangwood Metallurgical and materials transactions A 30, 2089-2096, 1999 | 83 | 1999 |
Effect of bimodal grain size distribution on scatter in toughness D Chakrabarti, M Strangwood, C Davis Metallurgical and Materials Transactions A 40, 780-795, 2009 | 81 | 2009 |