The effect of temperature and annealing on the phase composition, molecular mobility and the thickness of domains in high-density polyethylene C Hedesiu, DE Demco, R Kleppinger, AA Buda, B Blümich, K Remerie, ... Polymer 48 (3), 763-777, 2007 | 133 | 2007 |
One-pot synthesis of hyperbranched polyethoxysiloxanes X Zhu, M Jaumann, K Peter, M Möller, C Melian, A Adams-Buda, ... Macromolecules 39 (5), 1701-1708, 2006 | 119 | 2006 |
Domain sizes in heterogeneous polymers by spin diffusion using single-quantum and double-quantum dipolar filters A Buda, DE Demco, M Bertmer, B Blümich, B Reining, H Keul, H Höcker Solid state nuclear magnetic resonance 24 (1), 39-67, 2003 | 95 | 2003 |
Biodegradable shape-memory polymer networks: characterization with solid-state NMR M Bertmer, A Buda, I Blomenkamp-Höfges, S Kelch, A Lendlein Macromolecules 38 (9), 3793-3799, 2005 | 76 | 2005 |
Metal-free reduction of the greenhouse gas sulfur hexafluoride, formation of SF 5 containing ion pairs and the application in fluorinations M Rueping, P Nikolaienko, Y Lebedev, A Adams Green Chemistry, 2017 | 75 | 2017 |
Bifunctional nanoparticle–SILP catalysts (NPs@ SILP) for the selective deoxygenation of biomass substrates KL Luska, J Julis, E Stavitski, DN Zakharov, A Adams, W Leitner Chemical Science 5 (12), 4895-4905, 2014 | 70 | 2014 |
General analytical description of spin-diffusion for a three-domain morphology. Application to melt-spun nylon 6 fibers A Buda, DE Demco, M Bertmer, B Blümich, VM Litvinov, JP Penning The Journal of Physical Chemistry B 107 (22), 5357-5370, 2003 | 51 | 2003 |
Analysis of solid technical polymers by compact NMR A Adams TrAC Trends in Analytical Chemistry 83, 107-119, 2016 | 48 | 2016 |
Characterization of non-extractable 14C-and 13C-sulfadiazine residues in soil including simultaneous amendment of pig manure T Junge, KC Meyer, K Ciecielski, A Adams, A Schäffer, B Schmidt Journal of Environmental Science and Health, Part B 46 (2), 137-149, 2011 | 46 | 2011 |
Polyethylene/palygorskite nanocomposites: preparation by in situ polymerization and their characterization W Li, A Adams, J Wang, B Blümich, Y Yang Polymer 51 (21), 4686-4697, 2010 | 44 | 2010 |
Morphology of high-density polyethylene pipes stored under hydrostatic pressure at elevated temperature N Sun, M Wenzel, A Adams Polymer 55 (16), 3792-3800, 2014 | 42 | 2014 |
Understanding thermal aging of non-stabilized and stabilized polyamide 12 using 1 H solid-state NMR J Zhang, A Adams Polymer Degradation and Stability 134, 169-178, 2016 | 38 | 2016 |
Mobile NMR for analysis of polyethylene pipes B Blümich, F Casanova, A Buda, K Kremer, T Wegener Acta Physica Polonica A 108 (1), 13-23, 2005 | 38 | 2005 |
Complex Morphology of Melt-Spun Nylon-6 Fibres Investigated by 1H Double-Quantum-Filtered NMR Spin-Diffusion Experiments JPP A. Buda, D. E. Demco, B. Blümich, V. M. Litvinov ChemPhysChem 5 (6), 876-83, 2004 | 38 | 2004 |
Borazine-based inorganic–organic hybrid cyclomatrix microspheres by silicon/boron exchange precipitation polycondensation NA Riensch, A Deniz, S Kühl, L Müller, A Adams, A Pich, H Helten Polymer Chemistry, 2017 | 37 | 2017 |
Unilateral NMR and thermal microscopy studies of vegetable tanned leather exposed to dehydrothermal treatment and light irradiation E Badea, C Şendrea, C Carşote, A Adams, B Blümich, H Iovu Microchemical Journal 129, 158-165, 2016 | 35 | 2016 |
NON-INVASIVE CHARACTERISATION OF COLLAGEN-BASED MATERIALS BY NMR-MOUSE AND ATR-FTIR C SENDREA, C CARSOTE, E BADEA, A ADAMS, M NICULESCU, ... | 35* | |
Incorporation Mechanisms of a Branched Nonylphenol Isomer in Soil-Derived Organo–Clay Complexes during a 180-Day Experiment P Riefer, T Klausmeyer, A Adams, B Schmidt, A Schäffer, ... Environmental science & technology 47 (13), 7155-7162, 2013 | 32 | 2013 |
Nondestructive Quantification of Local Plasticizer Concentration in PVC by 1H NMR Relaxometry A Adams, R Kwamen, B Woldt, M Graß Macromolecular rapid communications 36 (24), 2171-2175, 2015 | 30 | 2015 |
Estimation of Self‐Diffusion Coefficients of Small Penetrants in Semicrystalline Polymers Using Single‐Sided NMR R Kwamen, B Blümich, A Adams Macromolecular rapid communications 33 (10), 943-947, 2012 | 29 | 2012 |