Electron-pinned defect-dipoles for high-performance colossal permittivity materials W Hu, Y Liu, RL Withers, TJ Frankcombe, L Norén, A Snashall, M Kitchin, ... Nature materials 12 (9), 821-826, 2013 | 884 | 2013 |
Phase perfection in zinc blende and wurtzite III− V nanowires using basic growth parameters HJ Joyce, J Wong-Leung, Q Gao, HH Tan, C Jagadish Nano letters 10 (3), 908-915, 2010 | 592 | 2010 |
Mechanical deformation in silicon by micro-indentation JE Bradby, JS Williams, J Wong-Leung, MV Swain, P Munroe Journal of Materials Research 16 (5), 1500-1507, 2001 | 290 | 2001 |
Selective-area epitaxy of pure wurtzite InP nanowires: high quantum efficiency and room-temperature lasing Q Gao, D Saxena, F Wang, L Fu, S Mokkapati, Y Guo, L Li, J Wong-Leung, ... Nano letters 14 (9), 5206-5211, 2014 | 254 | 2014 |
Transmission electron microscopy observation of deformation microstructure under spherical indentation in silicon JE Bradby, JS Williams, J Wong-Leung, MV Swain, P Munroe Applied Physics Letters 77 (23), 3749-3751, 2000 | 246 | 2000 |
Ultralow surface recombination velocity in InP nanowires probed by terahertz spectroscopy HJ Joyce, J Wong-Leung, CK Yong, CJ Docherty, S Paiman, Q Gao, ... Nano letters 12 (10), 5325-5330, 2012 | 206 | 2012 |
Gettering of copper to hydrogen‐induced cavities in silicon J Wong‐Leung, CE Ascheron, M Petravic, RG Elliman, JS Williams Applied physics letters 66 (10), 1231-1233, 1995 | 149 | 1995 |
Capture cross sections of the acceptor level of iron–boron pairs in p-type silicon by injection-level dependent lifetime measurements D Macdonald, A Cuevas, J Wong-Leung Journal of Applied Physics 89 (12), 7932-7939, 2001 | 146 | 2001 |
Indentation-induced damage in GaN epilayers JE Bradby, SO Kucheyev, JS Williams, J Wong-Leung, MV Swain, ... Applied Physics Letters 80 (3), 383-385, 2002 | 135 | 2002 |
High efficiency perovskite‐silicon tandem solar cells: effect of surface coating versus bulk incorporation of 2D perovskite T Duong, H Pham, TC Kho, P Phang, KC Fong, D Yan, Y Yin, J Peng, ... Advanced Energy Materials 10 (9), 1903553, 2020 | 129 | 2020 |
Enhanced minority carrier lifetimes in GaAs/AlGaAs core–shell nanowires through shell growth optimization N Jiang, Q Gao, P Parkinson, J Wong-Leung, S Mokkapati, S Breuer, ... Nano letters 13 (11), 5135-5140, 2013 | 123 | 2013 |
Ultra-micro-indentation of silicon and compound semiconductors with spherical indenters JS Williams, Y Chen, J Wong-Leung, A Kerr, MV Swain Journal of Materials Research 14 (6), 2338-2343, 1999 | 117 | 1999 |
Long minority carrier lifetime in Au-catalyzed GaAs/AlxGa1− xAs core-shell nanowires N Jiang, P Parkinson, Q Gao, S Breuer, HH Tan, J Wong-Leung, ... Applied Physics Letters 101 (2), 2012 | 116 | 2012 |
Mechanical deformation of InP and GaAs by spherical indentation JE Bradby, JS Williams, J Wong-Leung, MV Swain, P Munroe Applied Physics Letters 78 (21), 3235-3237, 2001 | 115 | 2001 |
Gettering of Au to dislocations and cavities in silicon J Wong‐Leung, E Nygren, JS Williams Applied physics letters 67 (3), 416-418, 1995 | 106 | 1995 |
Polarity-driven 3-fold symmetry of GaAs/AlGaAs core multishell nanowires C Zheng, J Wong-Leung, Q Gao, HH Tan, C Jagadish, J Etheridge Nano Letters 13 (8), 3742-3748, 2013 | 103 | 2013 |
Twinning superlattice formation in GaAs nanowires T Burgess, S Breuer, P Caroff, J Wong-Leung, Q Gao, H Hoe Tan, ... ACS nano 7 (9), 8105-8114, 2013 | 98 | 2013 |
Tunable Polarity in a III-V Nanowire by Droplet Wetting and Surface Energy Engineering. X Yuan, P Caroff, J Wong-Leung, L Fu, HH Tan, C Jagadish Advanced Materials (Deerfield Beach, Fla.) 27 (40), 6096-6103, 2015 | 91 | 2015 |
Nanoindentation-induced deformation of Ge JE Bradby, JS Williams, J Wong-Leung, MV Swain, P Munroe Applied physics letters 80 (15), 2651-2653, 2002 | 89 | 2002 |
Gettering of nickel to cavities in silicon introduced by hydrogen implantation B Mohadjeri, JS Williams, J Wong‐Leung Applied physics letters 66 (15), 1889-1891, 1995 | 88 | 1995 |