Mapping polymer heterogeneity using atomic force microscopy phase imaging and nanoscale indentation D Raghavan, X Gu, T Nguyen, M VanLandingham, A Karim Macromolecules 33 (7), 2573-2583, 2000 | 302 | 2000 |
Characterization of heterogeneous regions in polymer systems using tapping mode and force mode atomic force microscopy D Raghavan, M VanLandingham, X Gu, T Nguyen Langmuir 16 (24), 9448-9459, 2000 | 138 | 2000 |
Characterization of polyester degradation using tapping mode atomic force microscopy: exposure to alkaline solution at room temperature X Gu, D Raghavan, T Nguyen, MR VanLandingham, D Yebassa Polymer degradation and stability 74 (1), 139-149, 2001 | 110 | 2001 |
Free volumes, glass transitions, and cross-links in zinc oxide/waterborne polyurethane nanocomposites S Awad, H Chen, G Chen, X Gu, JL Lee, EE Abdel-Hady, YC Jean Macromolecules 44 (1), 29-38, 2011 | 106 | 2011 |
Statistical methods for degradation data with dynamic covariates information and an application to outdoor weathering data Y Hong, Y Duan, WQ Meeker, DL Stanley, X Gu Technometrics 57 (2), 180-193, 2015 | 93 | 2015 |
Fate of nanoparticles during life cycle of polymer nanocomposites T Nguyen, B Pellegrin, C Bernard, X Gu, JM Gorham, P Stutzman, ... Journal of Physics: Conference Series 304 (1), 012060, 2011 | 93 | 2011 |
Subsurface characterization of carbon nanotubes in polymer composites via quantitative electric force microscopy M Zhao, X Gu, SE Lowther, C Park, YC Jean, T Nguyen Nanotechnology 21 (22), 225702, 2010 | 84 | 2010 |
FTIR spectroscopy study of the formation of cyclic anhydride intermediates of polycarboxylic acids catalyzed by sodium hypophosphite G Xiaohong, CQ Yang Textile Research Journal 70 (1), 64-70, 2000 | 82 | 2000 |
Use of laser scanning confocal microscopy for characterizing changes in film thickness and local surface morphology of UV-exposed polymer coatings LP Sung, J Jasmin, X Gu, T Nguyen, JW Martin JCT research 1, 267-276, 2004 | 74 | 2004 |
C30 Self-Assembled Monolayers on Silica, Titania, and Zirconia: HPLC Performance, Atomic Force Microscopy, Ellipsometry, and NMR Studies of Molecular … M Pursch, DL Vanderhart, LC Sander, X Gu, T Nguyen, SA Wise, ... Journal of the American Chemical Society 122 (29), 6997-7011, 2000 | 73 | 2000 |
Linking accelerated laboratory test with outdoor performance results for a model epoxy coating system X Gu, D Stanley, WE Byrd, B Dickens, I Vaca-Trigo, WQ Meeker, ... Service Life Prediction of Polymeric Materials: Global Perspectives, 3-28, 2009 | 68 | 2009 |
Depth profiling of degradation of multilayer photovoltaic backsheets after accelerated laboratory weathering: Cross-sectional Raman imaging CC Lin, PJ Krommenhoek, SS Watson, X Gu Solar Energy Materials and Solar Cells 144, 289-299, 2016 | 66 | 2016 |
FT-IR and FT-Raman spectroscopy study of the cyclic anhydride intermediates for esterification of cellulose: I. Formation of anhydrides without a catalyst X Gu, CQ Yang Research on chemical intermediates 24, 979-996, 1998 | 63 | 1998 |
Microstructure and morphology of amine-cured epoxy coatings before and after outdoor exposures—an AFM study X Gu, T Nguyen, M Oudina, D Martin, B Kidah, J Jasmin, A Rezig, L Sung, ... JCT research 2, 547-556, 2005 | 62 | 2005 |
Effects of humidity and sample surface free energy on AFM probe− sample interactions and lateral force microscopy image contrast L Chen, X Gu, MJ Fasolka, JW Martin, T Nguyen Langmuir 25 (6), 3494-3503, 2009 | 55 | 2009 |
Surface and interfacial properties of PVDF/acrylic copolymer blends before and after UV exposure X Gu, CA Michaels, D Nguyen, YC Jean, JW Martin, T Nguyen Applied surface science 252 (14), 5168-5181, 2006 | 55 | 2006 |
Hole‐growth instability in the dewetting of evaporating polymer solution films X Gu, D Raghavan, JF Douglas, A Karim Journal of Polymer Science Part B: Polymer Physics 40 (24), 2825-2832, 2002 | 55 | 2002 |
Impact of environmental variables on the degradation of photovoltaic components and perspectives for the reliability assessment methodology Y Lyu, A Fairbrother, M Gong, JH Kim, X Gu, M Kempe, S Julien, KT Wan, ... Solar Energy 199, 425-436, 2020 | 54 | 2020 |
Differential degradation patterns of photovoltaic backsheets at the array level A Fairbrother, M Boyd, Y Lyu, J Avenet, P Illich, Y Wang, M Kempe, ... Solar Energy 163, 62-69, 2018 | 53 | 2018 |
Characterization of surface accumulation and release of nanosilica during irradiation of polymer nanocomposites by ultraviolet light T Nguyen, B Pellegrin, C Bernard, S Rabb, P Stuztman, JM Gorham, X Gu, ... Journal of Nanoscience and Nanotechnology 12 (8), 6202-6215, 2012 | 51 | 2012 |