Effects of UV degradation on surface hydrophobicity, crack, and thickness of MWCNT-based nanocomposite coatings R Asmatulu, GA Mahmud, C Hille, HE Misak Progress in Organic Coatings 72 (3), 553-561, 2011 | 145 | 2011 |
Galvanic corrosion of Al/Cu meshes with carbon fibers and graphene and ITO-based nanocomposite coatings as alternative approaches for lightning strikes B Zhang, VR Patlolla, D Chiao, DK Kalla, H Misak, R Asmatulu The International Journal of Advanced Manufacturing Technology 67, 1317-1323, 2013 | 88 | 2013 |
Skin cancer treatment by albumin/5-Fu loaded magnetic nanocomposite spheres in a mouse model H Misak, N Zacharias, Z Song, S Hwang, KP Man, R Asmatulu, SY Yang Journal of biotechnology 164 (1), 130-136, 2013 | 69 | 2013 |
Crack growth behavior of 7075-T6 under biaxial tension–tension fatigue HE Misak, VY Perel, V Sabelkin, S Mall International journal of fatigue 55, 158-165, 2013 | 67 | 2013 |
Functionalization of carbon nanotube yarn by acid treatment HE Misak, R Asmatulu, M O’Malley, E Jurak, S Mall International Journal of Smart and Nano Materials 5 (1), 34-43, 2014 | 66 | 2014 |
The addition of graphene to polymer coatings for improved weathering N Nuraje, SI Khan, H Misak, R Asmatulu International Scholarly Research Notices 2013 (1), 514617, 2013 | 64 | 2013 |
Environmental impacts of nanotechnology and its products B Zhang, H Misak, PS Dhanasekaran, D Kalla, R Asmatulu Proceedings of the 2011 Midwest Section Conference of the American Society …, 2011 | 58 | 2011 |
Thermal fatigue and hypothermal atomic oxygen exposure behavior of carbon nanotube wire HE Misak, V Sabelkin, S Mall, PE Kladitis Carbon 57, 42-49, 2013 | 47 | 2013 |
Tensile loading behavior of carbon nanotube wires V Sabelkin, HE Misak, S Mall, R Asmatulu, PE Kladitis Carbon 50 (7), 2530-2538, 2012 | 41 | 2012 |
Corrosion fatigue crack growth behavior of 7075-T6 under biaxial tension–tension cyclic loading condition HE Misak, VY Perel, V Sabelkin, S Mall Engineering Fracture Mechanics 106, 38-48, 2013 | 39 | 2013 |
Electrical conductivity, strength and microstructure of carbon nanotube multi-yarns HE Misak, S Mall Materials & Design 75, 76-84, 2015 | 32 | 2015 |
Biaxial tension–tension fatigue crack growth behavior of 2024-T3 under ambient air and salt water environments HE Misak, VY Perel, V Sabelkin, S Mall Engineering Fracture Mechanics 118, 83-97, 2014 | 32 | 2014 |
Albumin‐based nanocomposite spheres for advanced drug delivery systems HE Misak, R Asmatulu, JS Gopu, KP Man, NM Zacharias, PH Wooley, ... Biotechnology journal 9 (1), 163-170, 2014 | 32 | 2014 |
Failure in metal honeycombs manufactured by selective laser melting of 304 L stainless steel under compression S Anandan, RM Hussein, M Spratt, J Newkirk, K Chandrashekhara, ... Virtual and Physical Prototyping 14 (2), 114-122, 2019 | 31 | 2019 |
Hands-on nanotechnology experience in the college of engineering at WSU: A curriculum development R Asmatulu, H Misak Journal of Nano Education 3 (1-2), 13-23, 2011 | 30 | 2011 |
Tension–tension fatigue behavior of carbon nanotube wires HE Misak, R Asmatulu, V Sabelkin, S Mall, PE Kladitis Carbon 52, 225-231, 2013 | 29 | 2013 |
Investigation into crack initiation from corrosion pit in 7075-T6 under ambient laboratory and saltwater environments V Sabelkin, VY Perel, HE Misak, EM Hunt, S Mall Engineering Fracture Mechanics 134, 111-123, 2015 | 27 | 2015 |
Composite magnetic nanoparticle drug delivery system R Asmatulu, H Misak, S Yang, P Wooley US Patent 9,782,342, 2017 | 26 | 2017 |
Investigation into microstructure of carbon nanotube multi-yarn HE Misak, S Mall Carbon 72, 321-327, 2014 | 26 | 2014 |
Failure analysis of carbon nanotube wires HE Misak, V Sabelkin, S Mall, R Asmatulu, PE Kladitis Carbon 50 (13), 4871-4879, 2012 | 26 | 2012 |