Nanomaterials by severe plastic deformation: review of historical developments and recent advances K Edalati, A Bachmaier, VA Beloshenko, Y Beygelzimer, VD Blank, ... Materials Research Letters 10 (4), 163-256, 2022 | 339 | 2022 |
Influence of equal-channel angular pressing on precipitation in an Al–Zn–Mg–Cu alloy G Sha, YB Wang, XZ Liao, ZC Duan, SP Ringer, TG Langdon Acta Materialia 57 (10), 3123-3132, 2009 | 305 | 2009 |
Microstructure and corrosion properties of ultrafine-grained interstitial free steel B Hadzima, M Janeček, Y Estrin, HS Kim Materials Science and Engineering: A 462 (1-2), 243-247, 2007 | 191 | 2007 |
Newly developed Ti–Nb–Zr–Ta–Si–Fe biomedical beta titanium alloys with increased strength and enhanced biocompatibility I Kopova, J Stráský, P Harcuba, M Landa, M Janeček, L Bačákova Materials Science and Engineering: C 60, 230-238, 2016 | 189 | 2016 |
Evolution of defects in copper deformed by high-pressure torsion J Čížek, M Janeček, O Srba, R Kužel, Z Barnovská, I Procházka, ... Acta Materialia 59 (6), 2322-2329, 2011 | 142 | 2011 |
Surface treatment by electric discharge machining of Ti–6Al–4V alloy for potential application in orthopaedics P Harcuba, L Bačáková, J Stráský, M Bačáková, K Novotná, M Janeček Journal of the mechanical behavior of biomedical materials 7, 96-105, 2012 | 138 | 2012 |
Effect of ECAP processing on corrosion resistance of AE21 and AE42 magnesium alloys P Minárik, R Král, M Janeček Applied Surface Science 281, 44-48, 2013 | 124 | 2013 |
Mechanical properties and microstructure of a Mg alloy AZ31 prepared by equal-channel angular pressing M Janeček, M Popov, MG Krieger, RJ Hellmig, Y Estrin Materials Science and Engineering: A 462 (1-2), 116-120, 2007 | 119 | 2007 |
Work-hardening induced tensile ductility of bulk metallic glasses via high-pressure torsion SH Joo, DH Pi, ADH Setyawan, H Kato, M Janecek, YC Kim, S Lee, ... Scientific reports 5 (1), 9660, 2015 | 110 | 2015 |
Microstructure stability of ultra-fine grained magnesium alloy AZ31 processed by extrusion and equal-channel angular pressing (EX–ECAP) J Stráská, M Janeček, J Čížek, J Stráský, B Hadzima Materials Characterization 94, 69-79, 2014 | 108 | 2014 |
Increasing strength of a biomedical Ti-Nb-Ta-Zr alloy by alloying with Fe, Si and O J Stráský, P Harcuba, K Václavová, K Horváth, M Landa, O Srba, ... Journal of the mechanical behavior of biomedical materials 71, 329-336, 2017 | 105 | 2017 |
Effects of microstructure on mechanical properties of CuNiSi alloys M Gholami, J Vesely, I Altenberger, HA Kuhn, M Janecek, M Wollmann, ... Journal of Alloys and Compounds 696, 201-212, 2017 | 98 | 2017 |
Effect of microstructure on plastic deformation of Cu at low homologous temperatures Y Estrin, NV Isaev, SV Lubenets, SV Malykhin, AT Pugachov, ... Acta materialia 54 (20), 5581-5590, 2006 | 97 | 2006 |
Exceptional mechanical properties of ultra-fine grain Mg-4Y-3RE alloy processed by ECAP P Minárik, J Veselý, R Král, J Bohlen, J Kubásek, M Janeček, J Stráská Materials Science and Engineering: A 708, 193-198, 2017 | 90 | 2017 |
The development of vacancies during severe plastic deformation J Čížek, M Janeček, T Vlasák, B Smola, O Melikhova, D SV Materials transactions 60 (8), 1533-1542, 2019 | 85 | 2019 |
Evolution of microstructure and hardness in AZ31 alloy processed by high pressure torsion J Stráská, M Janeček, J Gubicza, T Krajňák, EY Yoon, HS Kim Materials Science and Engineering: A 625, 98-106, 2015 | 85 | 2015 |
Microstructure changes in a 2618 aluminium alloy during ageing and creep F Nový, M Janeček, R Král Journal of Alloys and Compounds 487 (1-2), 146-151, 2009 | 85 | 2009 |
Investigating deformation processes in AM60 magnesium alloy using the acoustic emission technique K Máthis, F Chmelík, M Janeček, B Hadzima, Z Trojanová, P Lukáč Acta materialia 54 (20), 5361-5366, 2006 | 85 | 2006 |
Influence of equal channel angular pressing routes on texture, microstructure and mechanical properties of extruded AX41 magnesium alloy T Krajňák, P Minárik, J Gubicza, K Máthis, R Kužel, M Janeček Materials Characterization 123, 282-293, 2017 | 82 | 2017 |
The effect of microstructure on fatigue performance of Ti–6Al–4V alloy after EDM surface treatment for application in orthopaedics J Stráský, M Janeček, P Harcuba, M Bukovina, L Wagner Journal of the mechanical behavior of biomedical materials 4 (8), 1955-1962, 2011 | 80 | 2011 |