A novel electrical contact material with improved self-lubrication for railway current collectors R Manory Wear 249 (7), 626-636, 2001 | 361 | 2001 |
Wear of railway contact wires against current collector materials RR Manory, N Grady Wear 215 (1-2), 146-155, 1998 | 201 | 1998 |
A sliding wear tester for overhead wires and current collectors in light rail systems R Manory, H Sinkis Wear 239 (1), 10-20, 2000 | 100 | 2000 |
The friction and wear of automotive grey cast iron under dry sliding conditions Part 1-relationships between wear loss and testing parameters M Terheci, RR Manory, JH Hensler Wear 180 (1-2), 73-78, 1995 | 67 | 1995 |
Carbon diffusion in uncoated and titanium nitride coated iron substrates during microwave plasma assisted chemical vapor deposition of diamond PS Weiser, S Prawer, A Hoffman, RR Manory, PJK Paterson, SA Stuart Journal of applied physics 72 (10), 4643-4647, 1992 | 67 | 1992 |
Proposal for a hardness measurement technique without indentor by gas-cluster-beam bombardment Z Insepov, R Manory, J Matsuo, I Yamada Physical Review B 61 (13), 8744, 2000 | 66 | 2000 |
The effects of MEVVA ion implantation on the tribological properties of PVD-TiN films deposited on steel substrates RR Manory, S Mollica, L Ward, KP Purushotham, P Evans, J Noorman, ... Surface and Coatings Technology 155 (2-3), 136-140, 2002 | 64 | 2002 |
Growth and structure control of films with cubic and tetragonal structures obtained by ion beam assisted deposition RR Manory, T Mori, I Shimizu, S Miyake, G Kimmel Journal of Vacuum Science & Technology A: Vacuum, Surfaces, and Films 20 (2 …, 2002 | 61 | 2002 |
Effect of grain size and test configuration on the wear behavior of alumina F Xiong, RR Manory, L Ward, M Terheci, S Lathabai Journal of the American Ceramic Society 80 (5), 1310-1312, 1997 | 54 | 1997 |
Tribological studies of Zr-implanted PVD TiN coatings deposited on stainless steel substrates KP Purushotham, LP Ward, N Brack, PJ Pigram, P Evans, H Noorman, ... Wear 254 (7-8), 589-596, 2003 | 53 | 2003 |
Compound layer growth and compound layer porosity of austenite plasma nitrocarburised non-alloyed steel S Li, RR Manory, JH Hensler Surface and Coatings Technology 71 (2), 112-120, 1995 | 53 | 1995 |
Effects of Deposition Parameters on Structure and Composition of Reactively Sputtered TiNx Films R Manory Surface Engineering 3 (3), 233-238, 1987 | 52 | 1987 |
HfO2 thin films prepared by ion beam assisted deposition T Mori, M Fujiwara, RR Manory, I Shimizu, T Tanaka, S Miyake Surface and Coatings Technology 169, 528-531, 2003 | 48 | 2003 |
Comparison of compound layer nucleation mechanisms in plasma nitriding and nitrocarburizing: the effect of CHn species S Li, RR Manory Journal of Materials Science 34, 1045-1049, 1999 | 45 | 1999 |
The effect of test parameters on alumina wear under low contact stress F Xiong, RR Manory Wear 236 (1-2), 240-245, 1999 | 44 | 1999 |
Chemically vapor deposited diamond films grown on titanium nitride coated and uncoated iron substrates PS Weiser, S Prawer, A Hoffman, PJK Paterson, RR Manory Journal of applied physics 76 (4), 2164-2168, 1994 | 42 | 1994 |
Modification of tribomechanical properties of commercial TiN coatings by carbon ion implantation LJ Liu, DK Sood, RR Manory, W Zhou Surface and Coatings Technology 71 (2), 159-166, 1995 | 40 | 1995 |
Correlation between crystalline perfection and film purity for chemically vapor deposited diamond thin films grown on fused quartz substrates S Prawer, A Hoffman, SA Stuart, R Manory, P Weiser, CS Lim, JM Long, ... Journal of applied physics 69 (9), 6625-6631, 1991 | 40 | 1991 |
Wear behaviour of CrN coatings MEVVA ion implanted with Zr KP Purushotham, LP Ward, N Brack, PJ Pigram, P Evans, H Noorman, ... Wear 257 (9-10), 901-908, 2004 | 37 | 2004 |
Mechanism and kinetics of tetrachlorosilane reactions in an argon‐hydrogen microwave plasma N Mayo, U Carmi, I Rosenthal, R Avni, R Manory, A Grill Journal of applied physics 55 (12), 4404-4412, 1984 | 37 | 1984 |