Toxic fluoride gas emissions from lithium-ion battery fires F Larsson, P Andersson, P Blomqvist, BE Mellander Scientific reports 7 (1), 10018, 2017 | 395 | 2017 |
Abuse by external heating, overcharge and short circuiting of commercial lithium-ion battery cells F Larsson, BE Mellander Journal of The Electrochemical Society 161 (10), A1611, 2014 | 311 | 2014 |
Characteristics of lithium-ion batteries during fire tests F Larsson, P Andersson, P Blomqvist, A Lorén, BE Mellander Journal of Power Sources 271, 414-420, 2014 | 292 | 2014 |
Current trends and future challenges of electrolytes for sodium-ion batteries K Vignarooban, R Kushagra, A Elango, P Badami, BE Mellander, X Xu, ... International Journal of Hydrogen Energy 41 (4), 2829-2846, 2016 | 264 | 2016 |
Effect of concentration and grain size of alumina filler on the ionic conductivity enhancement of the (PEO) 9LiCF3SO3: Al2O3 composite polymer electrolyte M Dissanayake, P Jayathilaka, RSP Bokalawala, I Albinsson, ... Journal of Power Sources 119, 409-414, 2003 | 249 | 2003 |
Ionic conductivity of plasticized (PEO)-LiCF3SO3 electrolytes L Bandara, M Dissanayake, BE Mellander Electrochimica acta 43 (10-11), 1447-1451, 1998 | 229 | 1998 |
Gas explosions and thermal runaways during external heating abuse of commercial lithium-ion graphite-LiCoO2 cells at different levels of ageing F Larsson, S Bertilsson, M Furlani, I Albinsson, BE Mellander Journal of power sources 373, 220-231, 2018 | 224 | 2018 |
Effect of TiO2 nano-filler and EC plasticizer on electrical and thermal properties of poly (ethylene oxide)(PEO) based solid polymer electrolytes K Vignarooban, M Dissanayake, I Albinsson, BE Mellander Solid State Ionics 266, 25-28, 2014 | 220 | 2014 |
Effect of plasticizers (EC or PC) on the ionic conductivity and thermal properties of the (PEO)9LiTf: Al2O3 nanocomposite polymer electrolyte system H Pitawala, M Dissanayake, VA Seneviratne, BE Mellander, I Albinson Journal of Solid State Electrochemistry 12, 783-789, 2008 | 185 | 2008 |
Dielectric relaxation, ionic conductivity and thermal studies of the gel polymer electrolyte system PAN/EC/PC/LiTFSI P Jayathilaka, M Dissanayake, I Albinsson, BE Mellander Solid State Ionics 156 (1-2), 179-195, 2003 | 161 | 2003 |
Theoretical approach on ceria-based two-phase electrolytes for low temperature (300–600° C) solid oxide fuel cells B Zhu, S Li, BE Mellander Electrochemistry Communications 10 (2), 302-305, 2008 | 155 | 2008 |
Lithium-ion battery aspects on fires in electrified vehicles on the basis of experimental abuse tests F Larsson, P Andersson, BE Mellander Batteries 2 (2), 9, 2016 | 154 | 2016 |
Ionic conductivity in poly (propylene glycol) complexed with lithium and sodium triflate I Albinsson, BE Mellander, JR Stevens The Journal of chemical physics 96 (1), 681-690, 1992 | 130 | 1992 |
Electrical conductivity and activation volume of the solid electrolyte phase -AgI and the high-pressure phase fcc AgI BE Mellander Physical Review B 26 (10), 5886, 1982 | 126 | 1982 |
Efficiency enhancement by mixed cation effect in dye-sensitized solar cells with PAN based gel polymer electrolyte M Dissanayake, CA Thotawatthage, GKR Senadeera, T Bandara, ... Journal of Photochemistry and Photobiology A: Chemistry 246, 29-35, 2012 | 117 | 2012 |
Electrolysis studies based on ceria-based composites B Zhu, I Albinsson, C Andersson, K Borsand, M Nilsson, BE Mellander Electrochemistry communications 8 (3), 495-498, 2006 | 114 | 2006 |
Thermal modelling of cell-to-cell fire propagation and cascading thermal runaway failure effects for lithium-ion battery cells and modules using fire walls F Larsson, J Anderson, P Andersson, BE Mellander Journal of the electrochemical society 163 (14), A2854, 2016 | 111 | 2016 |
New proton conducting membranes based on PVAL/H3PO2/H2O MA Vargas, RA Vargas, BE Mellander Electrochimica Acta 44 (24), 4227-4232, 1999 | 107 | 1999 |
Mobile charge carrier concentration and mobility of a polymer electrolyte containing PEO and Pr4N+ I− using electrical and dielectric measurements T Bandara, M Dissanayake, I Albinsson, BE Mellander Solid State Ionics 189 (1), 63-68, 2011 | 102 | 2011 |
Phase diagram and electrical conductivity of the Li2SO4-Li2CO3 system M Dissanayake, BE Mellander Solid State Ionics 21 (4), 279-285, 1986 | 96 | 1986 |