Mechanical alloying synthesis and bioactivity evaluation of nanocrystalline fluoridated hydroxyapatite MH Fathi, EM Zahrani Journal of Crystal Growth 311 (5), 1392-1403, 2009 | 182 | 2009 |
Fabrication and characterization of fluoridated hydroxyapatite nanopowders via mechanical alloying MH Fathi, EM Zahrani Journal of Alloys and Compounds 475 (1-2), 408-414, 2009 | 113 | 2009 |
In vitro bioactivity evaluation of magnesium-substituted fluorapatite nanopowders M Kheradmandfard, MH Fathi, M Ahangarian, EM Zahrani Ceramics International 38 (1), 169-175, 2012 | 81 | 2012 |
Molten salt induced corrosion of Inconel 625 superalloy in PbSO4-Pb3O4-PbCl2-Fe2O3-ZnO environment E Mohammadi Zahrani, AM Alfantazi Corrosion Science, 2012 | 78 | 2012 |
High temperature corrosion and electrochemical behavior of INCONEL 625 weld overlay in PbSO4–Pb3O4–PbCl2–CdO–ZnO molten salt medium EM Zahrani, AM Alfantazi Corrosion science 85, 60-76, 2014 | 76 | 2014 |
The effect of high-energy ball milling parameters on the preparation and characterization of fluorapatite nanocrystalline powder EM Zahrani, MH Fathi Ceramics International 35 (6), 2311-2323, 2009 | 75 | 2009 |
The effects of an inorganic corrosion inhibitor on the electrochemical behavior of superhydrophobic micro-nano structured Ni films in 3.5% NaCl solution AHN Nezhad, A Davoodi, EM Zahrani, R Arefinia Surface and Coatings Technology 395, 125946, 2020 | 57 | 2020 |
Surface modification of orthopedic implants by optimized fluorine-substituted hydroxyapatite coating: Enhancing corrosion behavior and cell function M Mansoorianfar, M Mansourianfar, M Fathi, S Bonakdar, M Ebrahimi, ... Ceramics International 46 (2), 2139-2146, 2020 | 47 | 2020 |
Hot corrosion of Inconel 625 overlay weld cladding in smelting off-gas environment E Mohammadi Zahrani, AM Alfantazi Metallurgical and Materials Transactions A 44, 4671-4699, 2013 | 38 | 2013 |
Novel fluorapatite/niobium composite coating for metallic human body implants MH Fathi, EM Zahrani, A Zomorodian Materials Letters 63 (13-14), 1195-1198, 2009 | 37 | 2009 |
Pitting of 316L stainless steel in flare piping of a petrochemical plant EM Zahrani, A Saatchi, A Alfantazi Engineering Failure Analysis 17 (4), 810-817, 2010 | 33 | 2010 |
Sol-gel derived nanocrystalline fluoridated hydroxyapatite powders and nanostructured coatings for tissue engineering applications E Mohammadi Zahrani, MH Fathi, AM Alfantazi Metallurgical and Materials Transactions A 42, 3291-3309, 2011 | 26 | 2011 |
Erosion-corrosion of electrodeposited superhydrophobic Ni-Al2O3 nanocomposite coatings under jet saline-sand slurry impingement AHN Nezhad, EM Zahrani, AM Alfantazi Corrosion Science, 110095, 2022 | 25 | 2022 |
Hot corrosion of Inconel 625 wrought alloy and weld overlay on carbon steel by gas metal arc welding in 47 PbSO4-23 ZnO-13 Pb3O4-7 PbCl2-5 CdO-5 Fe2O3 molten salt mixture EM Zahrani, AM Alfantazi Corrosion Science 183, 109348, 2021 | 24 | 2021 |
Tuning surface wettability of aluminum surface and its correlation with short and long term corrosion resistance in saline solutions E Khajavian, MR Attar, EM Zahrani, W Liu, A Davoodi, S Hosseinpour Surface and Coatings Technology 429, 127950, 2022 | 17 | 2022 |
Corrosion Behavior of Alloy 625 in PbSO4-Pb3O4-PbCl2-ZnO-10 Wt Pct CdO Molten Salt Medium E Mohammadi Zahrani, AM Alfantazi Metallurgical and Materials Transactions A 43, 2857-2868, 2012 | 17 | 2012 |
High temperature corrosion of 625 supperalloy under iron-zinc-lead oxide/sulfate/chloride salt mixtures EM Zahrani, C Cuevas-Arteaga, D Verhelst, A Alfantazi ECS Transactions 28 (24), 171, 2010 | 13 | 2010 |
Premature failure of grade-316Ti stainless steel tubing in a boiler feed-water heat exchanger in a steel complex E Mohammadi Zahrani Journal of Failure Analysis and Prevention 21 (1), 61-73, 2021 | 12 | 2021 |
The Effect of Rotation Speed and Time of Milling on Synthesisand Properties of Fluoridated Hydroxyapatite Biomaterial: Synthesis of fluorhydroxyapatite nanopowder MH Fathi, EM Zahrani Iranian Journal of Pharmaceutical Sciences 4 (3), 201-208, 2008 | 10 | 2008 |
Effect of novel thermal oxidation process on wear resistance of commercial pure titanium M Taheri, E Mohamadi Zahrani Surface engineering 24 (6), 475-478, 2008 | 8 | 2008 |