关注
Scott Williamson
标题
引用次数
引用次数
年份
Biomechanical evaluation of the less invasive stabilization system, angled blade plate, and retrograde intramedullary nail for the internal fixation of distal femur fractures
M Zlowodzki, S Williamson, PA Cole, LD Zardiackas, PJ Kregor
Journal of orthopaedic trauma 18 (8), 494-502, 2004
4282004
Surface roughness effects on the fatigue strength of additively manufactured Ti-6Al-4V
J Pegues, M Roach, RS Williamson, N Shamsaei
International Journal of Fatigue 116, 543-552, 2018
3022018
Fatigue life estimation of additive manufactured parts in the as‐built surface condition
JW Pegues, N Shamsaei, MD Roach, RS Williamson
Material Design & Processing Communications 1 (3), e36, 2019
782019
Tuning anatase and rutile phase ratios and nanoscale surface features by anodization processing onto titanium substrate surfaces
MD Roach, RS Williamson, IP Blakely, LM Didier
Materials Science and Engineering: C 58, 213-223, 2016
672016
Comparison of the corrosion fatigue characteristics of CP Ti-Grade 4, Ti-6Al-4V ELI, Ti-6Al-7Nb, and Ti-15Mo
MD Roach, RS Williamson, LD Zardiackas
ASTM International, 2005
562005
Surface modifications to enhance osseointegration–Resulting material properties and biological responses
KP Nobles, AV Janorkar, RS Williamson
Journal of Biomedical Materials Research Part B: Applied Biomaterials 109 …, 2021
542021
Fracture fixation with two locking screws versus three non-locking screws: a biomechanical comparison in a normal and an osteoporotic bone model
B Grawe, T Le, S Williamson, A Archdeacon, L Zardiackas
Bone & Joint Research 1 (6), 118-124, 2012
402012
Effect of duty cycle on the crystallinity, pore size, surface roughness and corrosion resistance of the anodized surface on titanium
RS Williamson, J Disegi, AV Janorkar, JA Griggs, MD Roach
Surface and Coatings Technology 277, 278-288, 2015
382015
Nanopore formation on the surface oxide of commercially pure titanium grade 4 using a pulsed anodization method in sulfuric acid
RS Williamson, J Disegi, JA Griggs, MD Roach
Journal of Materials Science: Materials in Medicine 24, 2327-2335, 2013
352013
Photofunctionalization of anodized titanium surfaces using UVA or UVC light and its effects against Streptococcus sanguinis
S Jain, RS Williamson, M Marquart, AV Janorkar, JA Griggs, MD Roach
Journal of Biomedical Materials Research Part B: Applied Biomaterials 106 (6 …, 2018
222018
Surface characterization, shear strength, and bioactivity of anodized titanium prepared in mixed-acid electrolytes
S Jain, RS Williamson, MD Roach
Surface and Coatings Technology 325, 594-603, 2017
192017
Effect of specimen surface area size on fatigue strength of additively manufactured Ti-6Al-4V parts
J Pegues, M Roach, RS Williamson, N Shamsaei
University of Texas at Austin, 2017
172017
Photocatalytic activity and antibacterial efficacy of UVA-treated titanium oxides
HA Johnson, RS Williamson, M Marquart, JD Bumgardner, AV Janorkar, ...
Journal of biomaterials applications 35 (4-5), 500-514, 2020
152020
Volume effects on the fatigue behavior of additively manufactured Ti-6Al-4V Parts
J Pegues, M Roach, RS Williamson, N Shamsaei
University of Texas at Austin, 2018
152018
Osteoblast response to nanostructured and phosphorus-enhanced titanium anodization surfaces
S Jain, RS Williamson, AV Janorkar, JA Griggs, MD Roach
Journal of Biomaterials Applications 34 (3), 419-430, 2019
132019
Comparison of Stress Corrosion Cracking of Ti-15Mo, Ti-6Al-7Nb, Ti-6Al-4V, and CP Ti
RS Williamson, MD Roach, LD Zardiackas
J. Test. Eval, 2004
92004
A comparison of the stress corrosion cracking susceptibility of commercially pure titanium grade 4 in Ringer's solution and in distilled water: A fracture mechanics approach
MD Roach, RS Williamson, JA Thomas, JA Griggs, LD Zardiackas
Journal of Biomedical Materials Research Part B: Applied Biomaterials 102 (1 …, 2014
82014
Anodized titanium with calcium and phosphorus surface enhancements for dental and orthopedic implant applications
J Nelson, S Jain, P Pal, HA Johnson, KP Nobles, AV Janorkar, ...
Thin Solid Films 745, 139117, 2022
62022
Comparison of the corrosion fatigue characteristics of 23Mn-21Cr-1Mo low nickel, 22Cr-13Ni-5Mn, and 18Cr-14Ni-2.5 Mo stainless steels
M Roach, R Williamson, L Zardiackas
Fatigue and Fracture of Medical Metallic Materials and Devices, 2007
62007
Comparison of stress corrosion cracking and corrosion fatigue (anodized and non-anodized grade 4 CP Ti)
LD Zardiackas, MD Roach, RS Williamson
ASTM International, 2006
52006