On the exceptionally high ductility of Mg–2Zn-0.3 Ca-0.2 Ce-0.1 Mn alloy

D Zhao, R Shi, P Evans, AA Luo, KY Xie - Materials Science and …, 2021 - Elsevier
A newly developed Mg–2Zn-0.3 Ca-0.2 Ce-0.1 Mn (in weight%, ZXEM2000) wrought alloy
exhibits an exceptionally high tensile ductility (29%±1.4% tensile elongation) along the …

Hot workability and microstructure of Mg–6.0 Zn–2.0 Yb–0.5 Zr magnesium alloy

C Liu, L Li, W Zhou, X Bai, H Zhong, Z Zhang… - Journal of Alloys and …, 2023 - Elsevier
Abstract Mg–6.0 Zn–2.0 Yb–0.5 Zr (wt%) alloy exhibits excellent strength and ductility
synergy after thermomechanical and heat treatment. Unfortunately, the hot workability and …

Origins of high ductility exhibited by an extruded magnesium alloy Mg-1.8 Zn-0.2 Ca: experiments and crystal plasticity modeling

J Wang, G Zhu, L Wang, E Vasilev, JS Park… - Journal of Materials …, 2021 - Elsevier
Low ductility and strength are major bottlenecks against Mg alloys' wide applications. In this
work, we systematically design the composition and fabrication process for a low-alloyed Mg …

Grain refinement and improved mechanical properties of Mg-4Zn-0.5 Ca-0.5 RE magnesium alloy by thermomechanical processing

M Maleki, S Berndorf, S Mohammadzehi… - Journal of Alloys and …, 2023 - Elsevier
Abstract The high strength Mg-4Zn-0.5 Ca-0.5 RE magnesium alloy was subjected to
different hot deformation processes of extrusion, forging, and their combination for grain …

[HTML][HTML] Hot compression behavior and microstructure evolution of Mg-Gd-Y-Zn-Zr alloy

X Chen, D Wang, Q Li, Y Xiong, K Tian… - Journal of Materials …, 2024 - Elsevier
In this work, the hot compression behavior and microstructure evolution of Mg-8Gd-3Y-xZn-
0.6 Zr (x= 0, 1.5) alloys were investigated by Gleeble-1500D thermal simulation test …

Microstructure evolution and mechanical properties of Mg-x% Zn-1% Mn (x= 4, 5, 6, 7, 8, 9) wrought magnesium alloys

DF Zhang, GL Shi, XB Zhao, FG Qi - … of Nonferrous Metals Society of China, 2011 - Elsevier
The roles of Zn content and thermo-mechanical treatment in affecting microstructures and
mechanical properties of Mg-x% Zn-1% Mn (mass fraction, x= 4, 5, 6, 7, 8, 9) wrought Mg …

Effects of fabrication methods on deformability and microstructure of Mg–Zn–Zr wrought alloy

KH Jung, YB Kim, GA Lee, Y Zhang… - … of Nonferrous Metals …, 2014 - Elsevier
The effects of fabrication processing methods on the workability of Mg–Zn–Zr wrought
magnesium alloy (ZK60A) were investigated based on the microstructure and inherent …

Microstructure, texture and mechanical properties of Mg–8Gd–4Y–1Nd–0.5 Zr alloy prepared by pre-deformation annealing, hot compression and ageing

Y Wu, H Xiong, Y Jia, S Xie, G Li - … of Nonferrous Metals Society of China, 2019 - Elsevier
Abstract An extruded Mg–8Gd–4Y–1Nd–0.5 Zr alloy was pre-heated at 470° C for 1 h and
subsequently compressed at 470° C and two strain rates of 0.2 and 0.0003 s–1 …

[HTML][HTML] Microstructural evolution, high temperature tensile deformation behavior, and deformation mechanism in an Mg–Zn–Y–Ca–Zr alloy processed by …

F Cao, R Liu, S Kong, N Guo, P Xu, G Xu - Journal of Materials Research …, 2023 - Elsevier
To explore high temperature ductility, a new Mg-2.70 Zn-1.34 Y-0.37 Ca-0.02 Zr (wt.%) alloy
has been fabricated by novel multidirectional forging (MDF) and hot rolling. The …

Hot deformation behavior of novel high-strength Mg-0.6 Mn-0.5 Al-0.5 Zn-0.4 Ca alloy

H Chen, Y Yang, C Hu, G Zhou, H Shi, G Jiang… - International Journal of …, 2023 - Springer
The hot compression behavior of as-extruded Mg-0.6 Mn-0.5 Al-0.5 Zn-0.4 Ca alloy was
studied on a Gleeble-3500 thermal simulation machine. Experiments were conducted at …