[HTML][HTML] Effects of Sm element addition on the workability and microstructure evolution of Mg-Gd-Y-Zr alloy during hot deformation

Y Pei, M Yuan, E Wei, B Teng - Materials & Design, 2023 - Elsevier
… the microstructure and mechanical properties of Mg alloys. … microstructure, improving the
strength and plasticity of the … -3Y-1Sm-0.5Zr (1Sm) alloy was developed. Hot compression …

[HTML][HTML] Hot compression behavior and microstructure evolution of Mg-Gd-Y-Zn-Zr alloy

X Chen, D Wang, Q Li, Y Xiong, K Tian… - Journal of Materials …, 2024 - Elsevier
… dynamic precipitation behavior in Mg-8.3Gd-2.6Y-0.4Zr alloy. … modify its microstructure and
mechanical characteristics [14]. … Mg-8Gd-3Y-xZn-0.6Zr alloy was developed, incorporating the …

Dynamic precipitation, dynamic recrystallization behavior, and microstructure evolution of the Mg–8.7 Gd–4.18 Y–0.42 Zr alloy during hot deformation

L Zhang, X Wu, X Zhang, X Yang, Y Li - Journal of Materials Science, 2022 - Springer
… hot workability of extruded Mg9.8Gd2.7Y0.4Zr alloy. It has … in microstructure and workability
of Mg–Gd–Y–Nd–Zr alloy … s −1 , the initial microstructure almost fully developed into the …

[HTML][HTML] Mechanical properties and microstructure evolution of Mg-Gd Alloy during aging treatment

Y Liu, Y Song, N Li, X Sha, M Xu, B Chen, B Gao… - Metals, 2021 - mdpi.com
… Li et al. produced a Mg-14Gd alloy with high tensile strength of 445 MPa after … evolution of
precipitations and their corresponding effect on the mechanical properties of a Mg-10Gd alloy

[HTML][HTML] Microstructure evolution and mechanical property of Mg-Gd-Y-Zn-Zr alloy wires prepared by hot drawing

Z Ling, M Chen, L Wang, K Ma, DD Zhang, Y Li… - Journal of Materials …, 2024 - Elsevier
… [10] produced AZ31 alloy wires with an average grain size of 9.6 μm by cold drawing, and
the dynamic recrystallisation induced by plastic deformation changed the initial homogeneous …

Effect of Nd Addition on the Microstructure, Precipitate and Mechanical Properties of Mg-Gd-Y-(Nd)-Zr Alloys

Z Gao, C Liu, S Jiang, Y Gao, Y Wan, Z Chen… - … Mechanical Properties of … - papers.ssrn.com
… Consequently, in this study, the Mg-7Gd-1Y-xNd-0.3Zr alloy was chosen to add 94 … , YS
Microstructural Evolution and Mechanical Properties of 672 Mg-9.8Gd-2.7Y-0.4Zr Alloy Produced

Dynamic recrystallization mechanism, texture evolution development and mechanical characteristics of a Mg–8.7 Gd–4.18 Y–0.42 Zr magnesium alloy by ECAP

L Zhang, Y Li - Progress in Natural Science: Materials International, 2024 - Elsevier
microstructural development and superplastic characteristic of a Mg–5Gd–4Y–0.4Zr alloy
produced … The microstructural evolution of the solution treatment GW94K (Mg–8.7Gd–4.18Y–…

[HTML][HTML] Synergistic effects of grain refinement and texture weakening on mechanical properties anisotropy of Mg-9Gd-4Y-2Zn-0.4 Zr alloy via RUE processing

Z Li, J Yu, D Lu, G Wu, Z Zhang, Q Zhang… - Journal of Materials …, 2022 - Elsevier
… In this paper, 3 passes RUE were applied to Mg-9Gd-4Y–2Zn-0.5Zr alloy to study the effect
Microstructural evolution and mechanical properties of Mg-9.8Gd-2.7Y-0.4Zr alloy produced

[HTML][HTML] Constitutive Model and Recrystallization Mechanism of Mg-8.7 Gd-4.18 Y-0.42 Zr Magnesium Alloy during Hot Deformation

L Zhang, X Wu, X Zhang, X Yang, Y Li - Materials, 2022 - mdpi.com
mechanical processes are indispensable parts of producing structural components with good
mechanical properties … and dynamic recrystallization of Mg-9.8Gd-2.7Y-0.4Zr alloy was the …

Effects of heat treatment before extrusion on dynamic recrystallization behavior, texture and mechanical properties of as-extruded Mg-Gd-Y-Zn-Zr alloy

M Li, Y Huang, Y Liu, X Wang, Z Wang - Materials Science and …, 2022 - Elsevier
… works and our results, it can be inferred that the Mg-9.8Gd-3.5Y-2.0Zn-0.4Zr (wt. %) …
Microstructural evolution and mechanical properties of Mg-9.8Gd-2.7Y-0.4Zr alloy produced by …