[HTML][HTML] Accelerated Spheroidization of Cementite in Sintered Ultrahigh Carbon Steel by Warm Deformation

P Nikiel, S Szczepanik, G Korpała - Metals, 2021 - mdpi.com
Evolution of microstructure and hardness in quenched ultrahigh carbon steel Fe-0.85 Mo-0.6
Si-1.4 C by warm compression on a Bähr plastometer-dilatometer at 775° C and at 0.001 to …

Accelerated Spheroidization of Cementite in Sintered Ultrahigh Carbon Steel by Warm Deformation.

P Nikiel, S Szczepanik, G Korpała… - Metals (2075 …, 2021 - search.ebscohost.com
Evolution of microstructure and hardness in quenched ultrahigh carbon steel Fe-0.85 Mo-0.6
Si-1.4 C by warm compression on a Bähr plastometer-dilatometer at 775 C and at 0.001 to 1 …

[PDF][PDF] Accelerated Spheroidization of Cementite in Sintered Ultrahigh Carbon Steel by Warm Deformation. Metals 2021, 11, 328

P Nikiel, S Szczepanik, G Korpała - 2021 - pdfs.semanticscholar.org
Evolution of microstructure and hardness in quenched ultrahigh carbon steel Fe-0.85 Mo-0.6
Si-1.4 C by warm compression on a Bähr plastometer-dilatometer at 775◦ C and at 0.001 to …