Development of high‐tenacity, high‐modulus poly (ethylene terephthalate) filaments via a next generation wet‐melt‐spinning process

JH Yoon, H Avci, M Najafi, L Nasri… - Polymer Engineering …, 2017 - Wiley Online Library
In this study, PET (intrinsic viscosity of 1.05 dl/g) was melt processed with a horizontal
isothermal bath (HIB) treatment. Tensile properties of PET fiber samples were highly …

Development of high-tenacity, high-modulus poly (ethylene terephthalate) filaments via a next generation wet-melt-spinning process

JH Yoon, H Avci, M Najafi, L Nasri… - Polymer Engineering …, 2017 - go.gale.com
In this study, PET (intrinsic viscosity of 1.05 dl/g) was melt processed with a horizontal
isothermal bath (HIB) treatment. Tensile properties of PET fiber samples were highly …

Development of High-Tenacity, High-Modulus Poly (ethylene terephthalate) Filaments via a Next Generation Wet-Melt-Spinning Process

J Yoon, H AVCI, M Najafi, L Nasri… - POLYMER …, 2017 - avesis.ogu.edu.tr
In this study, PET (intrinsic viscosity of 1.05 dl/g) was melt processed with a horizontal
isothermal bath (HIB) treatment. Tensile properties of PET fiber samples were highly …

Development of high‐tenacity, high‐modulus poly (ethylene terephthalate) filaments via a next generation wet‐melt‐spinning process

JH Yoon, H Avci, M Najafi, L Nasri, SM Hudson… - Polymer Engineering & …, 2017 - infona.pl
In this study, PET (intrinsic viscosity of 1.05 dl/g) was melt processed with a horizontal
isothermal bath (HIB) treatment. Tensile properties of PET fiber samples were highly …