FeCo/Pt (001) superlattices have been investigated experimentally. The strain was
controlled by varying the individual constituent thicknesses in the range 3–10 atomic
monolayers (ML), resulting in lattice-parameter ratios c/a between 1.18 and 1.31. The
sample with ac/a ratio of 1.18 has a preferred out-of-plane magnetization direction and
magnetic stripe domains, revealed by MFM, while samples with higher c/a ratios prefer in …