studied in the dependence on the deposition technology. The HVOF as-sprayed, laser
remelted HVOF sprayed and laser clad coatings were evaluated by SEM, XRD and ASTM G-
133 reciprocating sliding wear test. In dependence on used deposition technology, the
microstructure of coating varied namely in terms of grain size and phase composition. The
XRD analyses in the wear track revealed that the strain-induced fcc-to-hcp transformation is …