material which has inhomogeneity as a crack is studied using giant magnetoimpedance,
GMI, sensor. The sensor was moved by a specially designed moving system. The
amorphous (Co0. 94Fe0. 06) 72.5 Si12. 5B15 wire was used as a GMI sensor and 1 MHz
with 5 mA ac current applied to the GMI sensor. A large decrease in the output voltage of the
sensor circuit was observed when the sensor was moved on the top of the crack, after the …