that takes place during the solidification of a nickel-based superalloy. By combining
absorption and diffraction contrast imaging, deformation events could be classified by their
localization and permanence. In particular, a deformation mechanism arising from thermal
contraction in a temperature gradient was elucidated through digital image correlation. It
was concluded that this mechanism may explain the small misorientations typically …