by some processes production on physical characteristics of pellet form ration. The
experimental design had used a Randomized Completely Design with 4 x 3 factorial and 3
replocats. Factor A were processes production, ie: A0= without processing, A1= added 5%
water spraying, A2= added 5% hot water spraying and A3= steam 45 minute on 1000C and
pressure 1.7-1.8 kg/cm2. Factor R were added binder, ie: R0= control ration, R1= control …