has been fabricated from α-Si3N4, AlN, Al2O3 and Y2O3 starting powders, using gas
pressure sintering and three different sintering procedures. One series of samples was
heated up to 1825° C and then held for 3 h, another group of samples was held at a lower
temperature (1500 or 1600° C) for 1 h and then heated up to 1825° C and held for 3 h. The