X Qian, Z Dong, B Jiang, B Lei, H Yang, C He, L Liu… - Materials & Design, 2022 - Elsevier
… Mg-Zn alloy was found to exhibit high toughness and ductile fracture due to the segregation of Zn at grainboundary, the Mg-… Obvious strain partitioning is detected between the DRXed …
… In that context we also followed the kinetics of partitioning of … the grainboundaries, solute segregation to grainboundaries … on grainboundary precipitation in a model Al-Zn-Mg-Cu alloy …
… size, the maximum pole density in multiples of random distribution (mrd), the pole splitting width about RD in degree … The pole splitting is largest for AX101 and smallest for AZX2101. …
K Shimizu, H Toda, H Fujihara, K Hirayama… - Engineering Fracture …, 2019 - Elsevier
… Hydrogen trap sites in Al-Zn-Mg alloys used in this study are grainboundaries, dislocations, pores, vacancies, precipitate interfaces. In order to quantitatively analyze these trap site …
… grainboundary (GB) microchemistry and precipitation behaviour in high-strength Al-Zn-Mg-… , was systematically investigated in a model Al-Zn-Mg-Cu alloy of near AA7050 composition. …
… 2 Sn phase is the logical place for the Na to partition to after extrusion, … the grainboundaries, but in the grain interiors, it must be incorporated into the Mg 2 Sn particles when no Mg-Zn …
… of random density, MRD) with no significant splitting of the basal poles from the normal direction. … for other solutes (such as Zn) are found to be similar in both Mg and Al, and the close …
DW Kim, BC Suh, MS Shim, JH Bae, DH Kim… - … Materials transactions A, 2013 - Springer
… -oriented grains occurs, resulting in the texture having a splitting of … boundary.[43] On the other hand, it has been recently suggested that grainboundary mobility of RE-containing Mg …
… 4 a–b) of each partition indicates that the parent grains, elongated in the extrusion direction (ED), adopt a nearly perfect first order prismatic < 10 1 0 > -axis fiber texture. However, the …