… micropillars inside individual grains using a focused ion beam (FIB) system and compressing them … Different micropillarcompression tests were performed to quantify the effects of pillar …
… micropillarcompression tests on L-PBF 316L, Inconel718 (IN718), and DED 316L micropillars of varying diameters—but all single crystals compressed along <110> of the face …
… Microindentations, Vickers microhardness tests, and in-situ micropillarcompression tests were employed to measure the local mechanical properties (hardness and elastic modulus) at …
GF Tian, Y Chen, B Gan, Y Yang… - Materials Science Forum, 2019 - Trans Tech Publ
… and ductility information through micropillarcompression, and greatly improved the … on micropillarcompression coupled with EBSD technology in a polycrystalline nickel-base superalloy…
… presented and applied to an Inconel718 Ni-based superalloy. The mechanical behavior of … using two different strategies, micropillarcompression for the parameters defining the …
… Inconel718 is a Ni-based superalloy used in gas turbine … Inconel718 contains L1 2 -ordered Ni 3 (Al,lTi) γ′-phases, D0 … than in the micropillar, our preliminary results on the micropillar …
… , superalloys, and high entropy alloys (HEAs). To examine this aspect, micropillarcompression … In our prior micropillarcompression work on LPBF 316 L and IN718, which contain well-…
… As a member of the Nickel-based superalloys family, Inconel718 … solute segregation subjected to micro-pillarcompression. In the … Inconel718 alloy, determined by in-situ micro-pillar …