… of Al/ZnO NPs, their photocatalyticdegradation of methylorange (MO) dye was … photocatalytic activity compared to pristine ZnO under the visible light irradiation. This high degradation …
L Wang, Z Li, J Chen, Y Huang, H Zhang, H Qiu - Environmental Pollution, 2019 - Elsevier
… , 100% degradation of methylorange can be achieved within 150 min. The synergetic effect of photocatalysis and adsorption is main reason for excellent MO degradation of PG/ZnO …
P Jantawasu, T Sreethawong, S Chavadej - Chemical Engineering Journal, 2009 - Elsevier
… TiO 2 photocatalyst was synthesized by a sol–gel process with the aid of a structure-directing surfactant and employed for the photocatalyticdegradation of methylorange azo dye (…
L Ge, J Liu - Applied Catalysis B: Environmental, 2011 - Elsevier
… The photocatalytic activities of the QDs sensitized CdS-Bi 2 … by the photocatalyticdegradation of methylorange in an … of photocatalyst was added into 50 mL methylorange solution …
G Ganapathy Selvam, K Sivakumar - Applied Nanoscience, 2015 - Springer
… along with photocatalyticdegradation of methylorange dye. The … Photocatalyticdegradation of methylorange was measured … was found to be impressive in degradingmethylorange. …
L Lu, R Shan, Y Shi, S Wang, H Yuan - Chemosphere, 2019 - Elsevier
A series of TiO 2 /biochar composite catalysts were prepared by the hydrolysis method for the degradation of methylorange, where biochar was obtained from the pyrolysis of waste …
N Kislov, J Lahiri, H Verma, DY Goswami… - Langmuir, 2009 - ACS Publications
… To assess if the back side, ie, the dark side, of the crystal contributes to the photo degradation of methylorange, we also performed measurements with the back side covered with a …
Y Zhu, S Xu, D Yi - Reactive and Functional Polymers, 2010 - Elsevier
… methylorange (MeO) as a target pollutant, the adsorption capacities and the photocatalytic … enhances the photocatalyticdegradation activity for MeO under both UV and visible light. …
Z Jiang, F Yang, G Yang, L Kong, MO Jones… - … of Photochemistry and …, 2010 - Elsevier
… used for photocatalyticdegradation of methylorange. XRD, … for photo-degradation of methyl orange under visible light (>… for 6 h exhibiting superior photocatalytic performance in these …