Kinetics of densification and grain growth of pure tungsten during spark plasma sintering

Z Gao, G Viola, BEN Milsom, I Whitaker, H Yan… - … Materials Transactions B, 2012 - Springer
The kinetics of densification and grain growth of tungsten during spark plasma sintering
(SPS) was studied under isothermal conditions. The results show that using SPS, high …

Spark plasma sintering of pure tungsten powder: densification kinetics and grain growth

S Deng, T Yuan, R Li, F Zeng, G Liu, X Zhou - Powder Technology, 2017 - Elsevier
The densification kinetics and grain growth behavior of an undoped tungsten powder during
spark plasma sintering (SPS) were investigated under the pressure of 40 MPa and constant …

The effect of particle size on the densification kinetics of tungsten powder during spark plasma sintering

S Deng, J Li, R Li, H Zhao, T Yuan, L Li… - International Journal of …, 2020 - Elsevier
The influence of particle size on the densification kinetics of tungsten powder during spark
plasma sintering was investigated. The densification rate of tungsten powder in the …

Activated sintering of tungsten alloys through conventional and spark plasma sintering process

N Senthilnathan, A Raja Annamalai… - Materials and …, 2017 - Taylor & Francis
The sintering temperature of pure tungsten can be reduced through the addition of small
amounts of transition elements. The present study deals with the activated sintering of …

Densification mechanism and mechanical properties of tungsten powder consolidated by spark plasma sintering

G Lee, J McKittrick, E Ivanov, EA Olevsky - International Journal of …, 2016 - Elsevier
The dominant densification mechanism of a tungsten powder processed by spark plasma
sintering (SPS) is revealed by the continuum theory of sintering-based regression of the …

Effect of heating rate on densification and grain growth during spark plasma sintering of 93W-5.6 Ni-1.4 Fe heavy alloys

K Hu, X Li, S Qu, Y Li - Metallurgical and Materials Transactions A, 2013 - Springer
Blended 93W-5.6 Ni-1.4 Fe powders were sintered via the spark plasma sintering (SPS)
technique using heating rates from 10 K min− 1 to 380 K min− 1 (10° C min− 1 to 380° C …

Suppressing pore-boundary separation during spark plasma sintering of tungsten

J Ma, J Zhang, W Liu, Z Shen - Journal of nuclear materials, 2013 - Elsevier
A tungsten powder with bimodal particle size distribution is consolidated by spark plasma
sintering (SPS). Effects are made for understanding the densification and grain growth …

Plasma activated sintering (PAS) of tungsten powders

G Jones, JR Groza, K Yamazaki… - MATERIAL AND …, 1994 - Taylor & Francis
Abstract Plasma Activated Sintering (PAS) is a short time, high temperature densification
process based on three main contributions: resistance sintering, pressure application, and …

Densification mechanisms in spark plasma sintering: Effect of particle size and pressure

S Diouf, A Molinari - Powder technology, 2012 - Elsevier
Three particles size ranges (< 25, 25–45 and 45–90μm) of a commercial as-atomized
copper powder were used to study the effect on SPS mechanism of particle size, pressure …

Enhanced low-temperature sintering of tungsten

RM German, ZA Munir - Metallurgical Transactions A, 1976 - Springer
The effects of various transition metal additions on the sintering of a well-characterized, fine
tungsten powder were analyzed using both isothermal and constant heating rate …