Antioxidant efficiency of p-phenylenediamines in natural rubber vulcanizates

O Lorenz, CR Parks - Rubber Chemistry and Technology, 1961 - meridian.allenpress.com
… into the vulcanizates by means of a swelling technique. The vulcanizates were swollen in
a … After 72 hours at room temperature in this solution, the samples were removed, dried in …

The Effect of Temperature on the Air Aging of Rubber Vulcanizates

M Schoch, A Juve - … on Aging of Rubbers, 1949 - asmedigitalcollection.asme.org
temperature of exposure in an air aging test on the rate of deterioration of the properties of
typical vulcanizates of natural rubber, GR-S, GR-I, nitril rubber … is at room temperature or at an …

New understanding of microstructure formation of the rubber phase in thermoplastic vulcanizates (TPV)

H Wu, M Tian, L Zhang, H Tian, Y Wu, N Ning - Soft matter, 2014 - pubs.rsc.org
… Because the χ values are independent of temperature, the χ values of EPDM and PP at
170 C were determined at room temperature by contact angle method with a Dataphysics …

Influence of temperature on the tensile strength of carbon filled vulcanizates

RW Sambrook - Rubber Chemistry and Technology, 1971 - meridian.allenpress.com
… activated blacks, or reduction in hysteretic nature by heat treatment do not explain why
either should have so little effect at room temperature and yet so seriously impair high …

Synthesis and characterization of water swellable natural rubber vulcanizates

C Nakason, Y Nakaramontri, A Kaesaman… - European polymer …, 2013 - Elsevier
… h at room temperature, and then the mixture was aged for 24 h to allow it to reach equilibrium.
The mixture was then cast into 10 × 10 cm thin films and dried at room temperature for 24 …

Influence of sulphur crosslink type on the strain-induced crystallization of natural rubber vulcanizates during uniaxial stretching by in situ WAXD using a synchrotron …

W Sainumsai, K Suchiva, S Toki - Materials today: Proceedings, 2019 - Elsevier
… The rubber compounds were left at room temperature for 24 hours before testing. Vulcanization
was carried out in an electrically heated hydraulic press at 150C using the optimum cure …

ESR study of vulcanizates under the deformed state

J Funatsu, R Takagi, M Ito - Journal of applied polymer science, 2009 - Wiley Online Library
rubber matrix. When the ESR measurements for the stretched samples were carried out at
room temperature… In this study, swelling tests were carried out by toluene at room temperature

Identification of antioxidants in rubber vulcanizates

DW Carlson, MW Hayes, HC Ransaw… - Analytical …, 1971 - ACS Publications
… in base and oil-extended rubber and rubber vulcanízales. This paper describes a very fast
method for identifying a wide variety of rubber antioxidants by means of extraction followed by …

Effect of curing systems on selected physical properties of natural rubber vulcanizates

ML Studebaker - Rubber Chemistry and Technology, 1966 - meridian.allenpress.com
… In the present study, tensile strength was determined only at room temperature and at a
single rate, but the data can be used to construct a section of a failure envelope by plotting …

Influence of filler and cure systems on thermal aging resistance of natural rubber vulcanizates under strained condition

SS Choi, J Jose, MY Lyu, YI Huh… - Journal of applied …, 2010 - Wiley Online Library
… Kyunggi-do, Korea) for 24 h at room temperature to extract the free organic materials in the
sample… , Kyunggi-do, Korea) for 48 h at room temperature. After that, the weight of the swollen …