AJ Haider, A Jasim Mohammed, SS Shaker… - Energy …, 2017 - ui.adsabs.harvard.edu
Thermal evaporated Sn thin film was deposited followed by atmospheric oxidation annealing at 550 C for 1 h to fabricate nanostructured SnO 2 thin film sensor. The …
AJ Haider, AJ Mohammed, SS Shaker, KZ Yahya… - Energy Procedia, 2017 - infona.pl
Thermal evaporated Sn thin film was deposited followed by atmospheric oxidation annealing at 550° C for 1 h to fabricate nanostructured SnO2thin film sensor. The …
AJ Haider, AJ Mohammedb, SS Shakerc… - Energy …, 2017 - researchgate.net
Thermal evaporated Sn thin film was deposited followed by atmospheric oxidation annealing at 550oC for 1 h to fabricate nanostructured SnO2thin film sensor. The …
AJ Haider, AJ Mohammedb, SS Shakerc… - Energy …, 2017 - researchgate.net
Thermal evaporated Sn thin film was deposited followed by atmospheric oxidation annealing at 550oC for 1 h to fabricate nanostructured SnO2thin film sensor. The …