[HTML][HTML] Excess Mg in situ powder addition for enhancing critical current density of ex situ MgB2

NM Hapipi, SK Chen, AH Shaari, MMA Kechik, KP Lim… - Applied Physics A, 2022 - Springer
In this work, ex situ MgB2 bulks were added with (1.5 Mg+ 2B) and sintered in an attempt to
enhance its intergrain connectivity. The addition was varied within the range of 0–50 wt …

Excess Mg in situ powder addition for enhancing critical current density of ex situ MgB2

NM Hapipi, SK Chen, AH Shaari… - Applied Physics A …, 2022 - ui.adsabs.harvard.edu
In this work, ex situ MgB 2 bulks were added with (1.5 Mg+ 2B) and sintered in an attempt to
enhance its intergrain connectivity. The addition was varied within the range of 0-50 wt …

Excess Mg in situ powder addition for enhancing critical current density of ex situ MgB

NM Hapipi, AH Shaari, MMA Kechik, KP Lim… - Applied Physics. A …, 2022 - inis.iaea.org
[en] In this work, ex situ MgB 2 bulks were added with (1.5 Mg+ 2B) and sintered in an
attempt to enhance its intergrain connectivity. The addition was varied within the range of 0 …

Excess Mg in situ powder addition for enhancing critical current density of ex situ MgB2.

NM Hapipi, SK Chen, AH Shaari… - Applied Physics A …, 2022 - search.ebscohost.com
In this work, ex situ MgB< sub> 2 bulks were added with (1.5 Mg+ 2B) and sintered in an
attempt to enhance its intergrain connectivity. The addition was varied within the range of 0 …

Excess Mg in situ powder addition for enhancing critical current density of ex situ MgB2

NM Hapipi, SK Chen, AH Shaari… - Applied Physics A …, 2022 - shibaura.elsevierpure.com
In this work, ex situ MgB 2 bulks were added with (1.5 Mg+ 2B) and sintered in an attempt to
enhance its intergrain connectivity. The addition was varied within the range of 0–50 wt …

[PDF][PDF] Excess Mg in situ powder addition for enhancing critical current density of ex situ MgB 2

NM Hapipi, SK Chen, AH Shaari, MMA Kechik… - Applied Physics …, 2022 - academia.edu
In this work, ex situ MgB2 bulks were added with (1.5 Mg+ 2B) and sintered in an attempt to
enhance its intergrain connectivity. The addition was varied within the range of 0–50 wt …