A scalable bio-inspired polydopamine-Cu ion interfacial layer for high-performance lithium metal anode

Q Meng, H Zhang, Y Liu, S Huang, T Zhou, X Yang… - Nano Research, 2019 - Springer
The growth of Li dendrites and the instability of the solid electrolyte interphase (SEI) layer
during plating/stripping has hindered the practical application of high-energy-density …

A scalable bio-inspired polydopamine-Cu ion interfacial layer for high-performance lithium metal anode

Q Meng, H Zhang, Y Liu, S Huang, T Zhou, X Yang… - Nano …, 2019 - sciopen.com
The growth of Li dendrites and the instability of the solid electrolyte interphase (SEI) layer
during plating/stripping has hindered the practical application of high-energy-density …

A scalable bio-inspired polydopamine-Cu ion interfacial layer for high-performance lithium metal anode.

Q Meng, H Zhang, Y Liu, S Huang, T Zhou… - Nano …, 2019 - search.ebscohost.com
The growth of Li dendrites and the instability of the solid electrolyte interphase (SEI) layer
during plating/stripping has hindered the practical application of high-energy-density …

A scalable bio-inspired polydopamine-Cu ion interfacial layer for high-performance lithium metal anode

Q Meng, H Zhang, Y Liu, S Huang, T Zhou… - Nano …, 2019 - search.proquest.com
The growth of Li dendrites and the instability of the solid electrolyte interphase (SEI) layer
during plating/stripping has hindered the practical application of high-energy-density …

A scalable bio-inspired polydopamine-Cu ion interfacial layer for high-performance lithium metal anode

M Qianqian, H Zhang, Y Liu, S Huang… - Nano …, 2019 - search.proquest.com
The growth of Li dendrites and the instability of the solid electrolyte interphase (SEI) layer
during plating/stripping has hindered the practical application of high-energy-density …

A scalable bio-inspired polydopamine-Cu ion interfacial layer for high-performance lithium metal anode

Q Meng, H Zhang, Y Liu, S Huang, T Zhou, X Yang… - Nano …, 2019 - sciopen.com
The growth of Li dendrites and the instability of the solid electrolyte interphase (SEI) layer
during plating/stripping has hindered the practical application of high-energy-density …