(PM) process. With this aim, Ni–Ti and Co–Cr–Mo alloys powder was compacted into the
mould one by one with Co–Cr–Mo being the one side and Ni–Ti the other side. Then, Ni–Ti
side of the specimen was synthesised by self-propagating high temperature synthesis (SHS)
process. At the end of the SHS process (after the SHS process), the porous Ni–Ti alloy has
occurred. Finally, the specimen was sintered at 1050° C into argon atmosphere. Scanning …