Lattice strain evolution and load partitioning during creep of a Ni-based superalloy single crystal with rafted γ′ microstructure

J Coakley, D Ma, M Frost, D Dye, DN Seidman… - Acta materialia, 2017 - Elsevier
Acta materialia, 2017Elsevier
In-situ neutron diffraction measurements were performed on monocrystalline samples of the
Ni-based superalloy CMSX-4 during N-type γ′ raft formation under the tensile creep
conditions of 1150° C/100 MPa, and subsequently on a rafted sample under the low
temperature/high stress creep conditions of 715° C/825 MPa. During 1150° C/100 MPa
creep, the γ′ volume fraction decreased from∼ 70% to∼ 50%, the lattice parameter misfit
was partly relieved, and the load was transferred from the creeping γ matrix to the γ …
In-situ neutron diffraction measurements were performed on monocrystalline samples of the Ni-based superalloy CMSX-4 during N-type γ′ raft formation under the tensile creep conditions of 1150° C/100 MPa, and subsequently on a rafted sample under the low temperature/high stress creep conditions of 715° C/825 MPa. During 1150° C/100 MPa creep, the γ′ volume fraction decreased from∼ 70% to∼ 50%, the lattice parameter misfit was partly relieved, and the load was transferred from the creeping γ matrix to the γ′ precipitates. On cooling back to room temperature, a fine distribution of γ′ precipitates formed in the γ channels, and these precipitates were present in the 715° C/825 MPa creep regime. Under low temperature/high stress creep, the alloy with rafted γ′ microstructure exhibited superior creep strength to the cuboidal γ′ microstructure produced following a standard heat-treatment. A lengthy creep incubation period was observed, believed to be associated with {111}< 110> dislocations hindering propagation of {111}< 112> dislocations. Following the creep incubation period, extensive macroscopic creep strain accumulated during primary creep as the γ phase yielded. Finally, the diffraction data suggest a loss of precipitate/matrix coherency in the (0k0) interfaces as creep strain accumulated.
Elsevier
以上显示的是最相近的搜索结果。 查看全部搜索结果

Google学术搜索按钮

example.edu/paper.pdf
搜索
获取 PDF 文件
引用
References