Malaysian Rubber (SMR L). Two ranges of RH size were prepared, coarser size at 10-20
mm and fine size at 150-300 μm. While the RH loading was (10, 20, 30, 40 and 50 Phr). The
effects of RH on the tensile properties, physical properties and cure characteristics of the
compounds were examined. The results shown that the increasing of rice husk loading in