Highly aging-resistant elastomers doped with antioxidant-loaded clay nanotubes

Y Fu, D Zhao, P Yao, W Wang, L Zhang… - ACS Applied Materials …, 2015 - ACS Publications
A novel aging-resistant styrene–butadiene rubber (SBR) composite is prepared using the
antioxidant N-isopropyl-N′-phenyl-p-phenylenediamine (4010NA) loaded inside of …

Evaluation of practical applicability and synergistic effects of bio-based food packaging materials combined with plant-based stabilisers

T Havelt, S Brettschneider, M Schmitz - Processes, 2021 - mdpi.com
Different analyses and feasibility studies have been conducted on the plant extracts of thyme
(Thymus vulgaris), European horse chestnut (Aesculus hippocastanum), Nordmann fir …

Compatibility analysis between natural rubber/polybutadiene rubber and protective waxes based on experiments and materials studio simulations

S Jiang, Y Li, Z Yong - Journal of Applied Polymer Science, 2024 - Wiley Online Library
Protective waxes are typically mixtures of paraffin and microcrystalline waxes that retard the
aging of unsaturated rubbers and are widely used in rubber products. The wax solubility of …

Improving thermal-oxidative aging resistance of styrene-butadiene rubber by antioxidant loaded silica aerogel

XF Ping, Y Wang, L Liu, FY Liu, HW He, P Wang… - Chinese Journal of …, 2024 - Springer
The antioxidant N-isopropyl-N′-phenyl-p-phenylenediamine (4010NA) was dissolved in
ethanol and impregnated into silica aerogel (SAG) via vacuum-pressure cycles, yielding …

Effect of temperature on the extent of migration of low molecular weight moieties to rubber surface

R Torregrosa-Coque, S Álvarez-García… - International journal of …, 2011 - Elsevier
Vulcanized rubbers contain different low molecular weight additives in their formulation,
including antiozonants, plasticizers, oils, etc. These moieties–mostly paraffin wax–often …

Analysis of whitening phenomenon of EPDM article by humid aging

SS Choi, HS Chung, YT Joo, KM Yang… - Journal of applied …, 2012 - Wiley Online Library
An ethylene–propylene–diene terpolymer (EPDM) article used for a car component was
aged in 80° C humid air (60% relative humidity) for 30 days and in 80° C tap water for 7 …

Migration of low molecular weight moiety at rubber–polyurethane interface: An ATR-IR spectroscopy study

R Torregrosa-Coque, S Álvarez-García… - International journal of …, 2011 - Elsevier
In this study, a novel approach based on ATR-IR spectroscopy consisting in the combined
use of two prisms of different nature and refraction index (germanium—about 1μm depth and …

Analysis of the whitening phenomenon of a thermoplastic elastomer article by UV weathering

SS Choi, HS Chung, YT Joo, BK Min, SH Lee - Polymer testing, 2011 - Elsevier
A thermoplastic elastomer (TPE) article composed of polypropylene (PP) and ethylene-
propylene-diene terpolymer (EPDM) was weathered by exposure to UV radiation of …

Influence of solvent swell and bound rubber on wax solubility of carbon black‐reinforced NR composite

SS Choi, SH Im, C Nah - Journal of Applied Polymer Science, 2012 - Wiley Online Library
Wax in a rubber article migrates to the surface and plays the role of an antidegradant by
formation of an impervious barrier on the surface. Wax solubility of a rubber article is …

Migration of Paraffin Wax to Sulfur Vulcanized Styrene–Butadiene Rubber (SBR) Surface: Effect of Temperature

R Torregrosa-Coque, S Álvarez-García… - Journal of Adhesion …, 2012 - Taylor & Francis
Because of the low molecular weight of some additives (eg, antiozonants) in the vulcanized