Ultrahigh cryogenic strength and exceptional ductility in ultrafine-grained CoCrFeMnNi high-entropy alloy with fully recrystallized structure

SJ Sun, YZ Tian, XH An, HR Lin, JW Wang… - Materials Today Nano, 2018 - Elsevier
Similar to the conventional alloys, attaining excellent combination of high strength and
ductility is still challenging in the high-entropy alloys (HEAs). In this work, a fully …

In-situ formed oxide enables extraordinary high-cycle fatigue resistance in additively manufactured CoCrFeMnNi high-entropy alloy

YK Kim, MS Baek, S Yang, KA Lee - Additive Manufacturing, 2021 - Elsevier
The high-cycle fatigue (HCF) properties and deformation behavior of additively
manufactured equiatomic CoCrFeMnNi high-entropy alloys (HEAs), strengthened by in-situ …

Superior low-cycle fatigue properties of CoCrNi compared to CoCrFeMnNi

K Lu, A Chauhan, M Walter, AS Tirunilai, M Schneider… - Scripta Materialia, 2021 - Elsevier
We report on the low-cycle fatigue behavior of single-phase, face-centered cubic CoCrNi
and CoCrFeMnNi at room temperature. Both alloys manifest cyclic hardening followed by …

Grain size and scratching depth dependent tribological characteristics of CrCoNi medium-entropy alloy coatings: a molecular dynamics simulation study

J Zhang, G Deng, W Li, S Li, Y Yan, X Liu, T Ma… - Surface and Coatings …, 2023 - Elsevier
In this work, we have investigated the impact of grain size and scratching depth on the
tribological behavior of nanocrystalline CrCoNi medium-entropy alloy (MEA) coatings during …

[HTML][HTML] High-cycle fatigue induced twinning in CoCrFeNi high-entropy alloy processed by laser powder bed fusion additive manufacturing

Y Chen, B Li, B Chen, F Xuan - Additive Manufacturing, 2023 - Elsevier
Abstract High-cycle fatigue (R= 0.1, room temperature) induced microstructural evolution in
a laser powder bed fusion (L-PBF) additively manufactured quaternary CoCrFeNi high …

Temperature dependence of the Hall–Petch relationship in CoCrFeMnNi high-entropy alloy

SJ Sun, YZ Tian, HR Lin, XG Dong, YH Wang… - Journal of Alloys and …, 2019 - Elsevier
Single-phase equiatomic CoCrFeMnNi high-entropy alloy (HEA) specimens with three
different grain sizes (0.65 μm, 2.1 μm and 105 μm) were processed by cold rolling and …

Microstructure, mechanical and tribological properties of Al0. 3CrFeNiTi0. 3-CaF2/BaF2 self-lubricating composite fabricated by spark plasma sintering

C Nguyen, AK Tieu, L Su, X Wu, TD Vo, L Wang… - Tribology …, 2023 - Elsevier
In this study, a bulk solid Al 0.3 CrFeNiTi 0.3-CaF 2/BaF 2 (HEA-CaF 2/BaF 2) self-
lubricating composite was successfully fabricated using spark-plasma sintering (SPS) …

Deformation mechanisms of CoCrFeMnNi high-entropy alloy under low-cycle-fatigue loading

K Lu, A Chauhan, AS Tirunilai, J Freudenberger… - Acta Materialia, 2021 - Elsevier
Plastic deformation during low-cycle fatigue (LCF) in equiatomic face-centered cubic (FCC)
CoCrFeMnNi high-entropy alloys (HEAs) is accumulated by dislocation substructure …

Mechanism of dislocation evolution during plastic deformation of nitrogen-doped CoCrFeMnNi high-entropy alloy

Y Han, H Li, H Feng, Y Tian, Z Jiang, T He - Materials Science and …, 2021 - Elsevier
In this study, the evolution of statistically stored dislocation (SSD) and geometrically
necessary dislocation (GND) during tensile tests was investigated in CoCrFeMnNi high …

Effect of the grain size on the corrosion behavior of CoCrFeMnNi HEAs in a 0.5 M H2SO4 solution

Y Wang, J Jin, M Zhang, X Wang, P Gong… - Journal of Alloys and …, 2021 - Elsevier
This work investigated the corrosion behavior of the equiatomic CoCrFeMnNi high entropy
alloy (HEA) in a 0.5 MH 2 SO 4 solution. The grain size of the HEA was adjusted by …