Modelling impact fracture and fragmentation of laminated glass using the combined finite-discrete element method

X Chen, AHC Chan - International Journal of Impact Engineering, 2018 - Elsevier
Fracture and fragmentation responses of laminated glass under hard body impact are
modelled with the combined finite-discrete element method (FEM-DEM). The method is …

Enhancement of hardness, modulus and fracture toughness of the tetragonal (Fe, Cr) 2B and orthorhombic (Cr, Fe) 2B phases with addition of Cr

J Lentz, A Röttger, F Großwendt, W Theisen - Materials & Design, 2018 - Elsevier
This study analyzes the influence of Cr content on hardness H, elastic modulus E and
fracture toughness K IC of the M 2 B boride by means of nanoindentation experiments …

Young's modulus and hardness of multiphase CaZrO3-MgO ceramics by micro and nanoindentation

AP Silva, F Booth, L Garrido, E Aglietti, P Pena… - Journal of the European …, 2018 - Elsevier
The aim of this work is to determine the values of the hardness and elastic modulus of the
phases present in CaZrO 3-MgO-ZrO 2 composites and to analyse their contribution to the …

The mechanical response characteristics of sapphire under dynamic and quasi-static indentation loading

X Luan, F Jiang, N Wang, X Xu, X Lu, Q Wen - Ceramics International, 2018 - Elsevier
Sapphire is widely used as optical materials and substrate materials due to its excellent
physical and chemical properties. The mechanism of crack propagation and fracture …

Indentation and bending behavior of electroless Ni-P-Ti composite coatings on pipeline steel

C Wang, Z Farhat, G Jarjoura, MK Hassan… - Surface and coatings …, 2018 - Elsevier
Electroless Ni-P coatings have been adopted in many industrial applications due to their
excellent wear and corrosion resistance. The unique properties and autocatalytic nature …

Adhesive-deformation relationships and mechanical properties of nc-AlCrN/a-SiNx hard coatings deposited at different bias voltages

M Haršáni, N Ghafoor, K Calamba, P Zacková, M Sahul… - Thin Solid Films, 2018 - Elsevier
A series of Al-Cr-Si-N hard coatings were deposited on WC-Co substrates with a negative
substrate bias voltage ranging from− 50 to− 200 V using cathodic arc evaporation system. A …

Back-Spalling process of an Al2O3 ceramic plate subjected to an impact of steel ball

Y Zhu, GR Liu, Y Wen, C Xu, W Niu, G Wang - International Journal of …, 2018 - Elsevier
Back-spalling of ceramic plates subjected to an impact is often observed phenomena, and a
better understanding of back-spalling is critical for the design of protection systems …

Local strain distribution and microstructure of grinding-induced damage layers in SiC wafer

S Tsukimoto, T Ise, G Maruyama, S Hashimoto… - Journal of Electronic …, 2018 - Springer
The high-angular-resolution electron backscatter diffraction (HR-EBSD) technique has been
utilized to evaluate the elastic strain distribution of grinding-induced damage layers in silicon …

[HTML][HTML] Investigation of local deformation behaviour of metallic materials and recent research trends: a review

M Lee, JB Jeon, TS Jun - Korean Journal of Metals and Materials, 2018 - kjmm.org
The behaviour and performance of complex metallic materials (eg, advanced high strength
steel and dual phase Ti alloys) are acknowledged to be multi-scale in nature and to rely on …

New insights into nanoindentation crack initiation in ion‐exchanged sodium aluminosilicate glass

X Li, L Jiang, I Mohagheghian, JP Dear… - Journal of the …, 2018 - Wiley Online Library
The effect of ion‐exchange on the fracture behavior and the threshold load is investigated
for radial crack initiation resulting from cube‐corner indentation. Both tin and air sides of the …