Observation of cavitation governing fracture in glasses

LQ Shen, JH Yu, XC Tang, BA Sun, YH Liu, HY Bai… - Science …, 2021 - science.org
Crack propagation is the major vehicle for material failure, but the mechanisms by which
cracks propagate remain longstanding riddles, especially for glassy materials with a long …

Nanoscale periodic distribution of energy dissipation at the shear band plane in a Zr-based metallic glass

DP Wang, HT Zhang, PY Guo, BA Sun, YX Wang - Scripta Materialia, 2021 - Elsevier
The local energy dissipation near the shear band plane was characterized by using a
method of amplitude-modulation atomic force microscope, in a Cu 50 Zr 50 metallic glass …

Flaw-insensitive fracture of a micrometer-sized brittle metallic glass

R Qu, R Maaß, Z Liu, D Tönnies, L Tian, RO Ritchie… - Acta Materialia, 2021 - Elsevier
Brittle materials, such as oxide glasses, are usually very sensitive to flaws, giving rise to a
macroscopic fracture strength that is much lower than that predicted by theory. The same …

Intrinsic and extrinsic effects on the fracture toughness of ductile metallic glasses

H Li, QX Pei, ZD Sha, PS Branicio - Mechanics of Materials, 2021 - Elsevier
The potential application of metallic glasses (MGs) as structural materials demands accurate
measurements of their toughness and the understanding of the underlying factors affecting …

Effect of strain rate and extrinsic size effect on micro-mechanical properties of zr-based bulk metallic glass

T Tabbakh, A Kurdi, AK Basak - Metals, 2021 - mdpi.com
In this study, the mechanical properties and deformation features of Zr-based bulk metallic
glass (BMG) are investigated at micro-scale via in situ micro-pillar compression …

[HTML][HTML] Research progress in shear banding deformation and fracture mechanisms of metallic glasses

R QU, X WANG, S WU, Z ZHANG - Acta Metall Sin, 2021 - ams.org.cn
Plastic deformation of metallic glasses (MGs) at room temperature usually localizes into
shear bands. The shear banding behavior dominates the deformation and fracture …

[PDF][PDF] 金属玻璃的剪切带变形与断裂机制研究进展

屈瑞涛, 王晓地, 吴少杰, 张哲峰 - 金属学报, 2021 - researchgate.net
摘要金属玻璃的室温塑性变形一般高度局域于剪切带中, 因此剪切带行为主导着金属玻璃的变形
与断裂机制, 对力学性能(如强度, 塑性, 韧性及疲劳性能等) 有重要影响. 鉴于剪切带行为对理解 …

Stretching the Limits in Thermoplastic Forming of Bulk Metallic Glasses

RM Ojeda Mota - 2021 - elischolar.library.yale.edu
Metallic glasses (MG) suggest that superb mechanical properties can be paired with plastic-
like processing. Their high strength and elasticity are often paired with fracture toughness …

[图书][B] Stretching the Limits in Thermoplastic Forming of Bulk Metallic Glasses

RMO Mota - 2021 - search.proquest.com
Metallic glasses (MG) suggest that superb mechanical properties can be paired with plastic-
like processing. Their high strength and elasticity are often paired with fracture toughness …

Sinterizzazione e analisi della microstruttura di leghe raffreddate rapidamente= Sintering and microstructure analysis of rapidly cooled alloys

S Xing - 2021 - webthesis.biblio.polito.it
I vetri metallici massicci a base di ferro (BMG) sono stati ampiamente studiati per le loro
potenziali applicazioni tecnologiche e le loro interessanti proprietà fisiche e meccaniche …