Corrosion mechanisms in molten salt thermal energy storage for concentrating solar power

S Bell, T Steinberg, G Will - Renewable and Sustainable Energy Reviews, 2019 - Elsevier
High temperature corrosion of molten salt containment materials is of great interest for
thermal energy storage systems used with concentrating solar power. Mitigating this …

Materials compatibility for the next generation of Concentrated Solar Power plants

M Sarvghad, SD Maher, D Collard, M Tassan… - Energy Storage …, 2018 - Elsevier
The next generation of Concentrated Solar Power (CSP) plants are expected to operate at
higher temperatures than those currently in use, for improved efficiency and reduced cost of …

High-temperature corrosion behavior of superalloys in molten salts–a review

NS Patel, V Pavlík, M Boča - Critical Reviews in Solid State and …, 2017 - Taylor & Francis
The use of molten salts based on fluorides/chlorides/nitrates/sulfates or carbonates is now
an accepted practice in energy conversion technologies and many other industrial …

Hot oxidation and corrosion behaviour of boiler steel fabricated by wire arc additive manufacturing

AR Kannan, CD Prasad, V Rajkumar… - Materials …, 2023 - Elsevier
Boiler Steels undergo severe degradation in corrosion resistance due to oxide scale
formation at elevated temperatures. In this study, the comparative hot oxidation and hot …

Investigations on the microstructure, tensile strength and high temperature corrosion behaviour of Inconel 625 and Inconel 718 dissimilar joints

KD Ramkumar, WS Abraham, V Viyash… - Journal of Manufacturing …, 2017 - Elsevier
In this article, an attempt has been made to investigate the effect of fillers on the pulsed
current gas tungsten arc welding (PCGTAW) of Inconel 625 and Inconel 718. Two different …

Microstructure, mechanical properties and corrosion behavior of laser welded dissimilar joints between ferritic stainless steel and carbon steel

W Wu, S Hu, J Shen - Materials & Design (1980-2015), 2015 - Elsevier
The joint of dissimilar metals between ferritic stainless steel (FSS) and low carbon steel (CS)
are welded by laser beam with two different welding speeds: 12 mm/s and 24 mm/s …

Microstructures and mechanical properties of dissimilar T91/347H steel weldments

R Mittal, BS Sidhu - Journal of Materials Processing Technology, 2015 - Elsevier
Shielded metal arc welding (SMAW), gas tungsten arc welding (GTAW) and their
combination are processed by using austenitic and nickel based diverse welding …

Effect of filler materials on the performance of gas tungsten arc welded AISI 304 and Monel 400

KD Ramkumar, N Arivazhagan, S Narayanan - Materials & Design, 2012 - Elsevier
Dissimilar metal welding involving AISI 304 and Monel 400 finds widespread use in marine
and offshore environments for the fabrication of heat exchangers, evaporators, piping and …

Dissimilar joining of AISI 304L/St37 steels by TIG welding process

AR Khalifeh, A Dehghan, E Hajjari - Acta Metallurgica Sinica (English …, 2013 - Springer
In present work the weldings of an austenitic stainless steel (AISI 304L) and a ferritic carbon
steel (St37) were conducted by tungsten inert gas (TIG) welding process using four different …

Erosive wear performance of heat treated multi-component cast iron containing Cr, V, Mn and Ni eroded by alumina spheres at elevated temperatures

Y Zhang, K Shimizu, X Yaer, K Kusumoto… - Wear, 2017 - Elsevier
Due to the urgent demand for the development of new materials with high performance and