Bulk hot deformation is a relatively old manufacturing technique widely adopted in different industry fields to form and shape different metallic alloys. Martensitic stainless steels (MSS) …
The effect of microstructural features on the hydrogen induced cracking (HIC) susceptibility of two API 5L X65 pipeline steels were investigated by cathodic charging, hydrogen …
MA Kappes, T Perez - Corrosion Reviews, 2023 - degruyter.com
Existing natural gas pipelines provide an economic alternative for the transport of hydrogen (H2) in an envisioned hydrogen economy. Hydrogen can dissolve in the steel and cause …
H Niazi, R Eadie, W Chen, H Zhang - Engineering Failure Analysis, 2021 - Elsevier
Abstract High pH Stress Corrosion Cracking (HpHSCC) was identified in the 1960 s for the first time and is considered to be a significant threat for buried pipelines. When certain …
The evolution of the microstructure changes during hot deformation of high-chromium content of stainless steels (martensitic stainless steels) is reviewed. The microstructural …
M Röthig, J Hoschke, C Tapia, J Venezuela… - International Journal of …, 2024 - Elsevier
The addition of small amounts of certain gases, such as O 2, CO, and SO 2, may mitigate hydrogen embrittlement in high-pressure gas transmission pipelines that transport …
R Ramesh, I Dinaharan, R Ravikumar… - Materials Science and …, 2020 - Elsevier
Laser beam welding (LBW) has many advantages to join high strength low alloy (HSLA) steels compared with conventional fusion welding processes. The present work is focused …
T Schaupp, W Ernst, H Spindler… - International journal of …, 2020 - Elsevier
High-strength steels with yield strength of 960 MPa are susceptible to hydrogen-assisted cracking (HAC) during welding processing. In the present paper, the implant test is used to …
This review paper concerns the development of the chemical compositions and controlled processes of rolling and cooling steels to increase their mechanical properties and reduce …