Cavitation erosion behavior of high velocity oxy fuel (HVOF) sprayed (VC+ CuNi-Cr) based novel coatings on SS316 steel

V Singh, I Singh, A Bansal, A Omer, AK Singla… - Surface and Coatings …, 2022 - Elsevier
A well-known hard material (VC) has not been explored as potential candidate for surface
modifications to overcome the problem of cavitation erosion (CE) in hydro machinery …

Development, characterization, and cavitation erosion analysis of high velocity oxy-fuel (HVOF) sprayed TiC and (70Cu-30Ni)-Cr based composite coatings on SS316 …

AK Singla, A Bansal, V Singh, N Khanna, DK Goyal… - Tribology …, 2023 - Elsevier
A novel composite coating was developed by depositing powders of Titanium Carbide (TiC)
with Cupronickel (70Cu-30Ni) and Chromium (Cr) as binders onto SS316 steel specimens …

Influence of thickness of hydrophobic polytetrafluoroethylene (PTFE) coatings on cavitation erosion of hydro-machinery steel SS410

A Bansal, J Singh, H Singh, DK Goyal - Wear, 2021 - Elsevier
Hydrophobic materials have the potential to replace the existing surface modification
materials to combat the problem of cavitation erosion (CE), owing to their various …

Effect of fuel pressure, feed rate, and spray distance on cavitation erosion of Rodojet sprayed Al2O3+ 50% TiO2 coated AISI410 steel

S Pandey, A Bansal, A Omer, AK Singla… - Surface and Coatings …, 2021 - Elsevier
Cavitation erosion is one of the major concerns of wear in hydro-machinery. The ensuing
damage can be mitigated by using protective coatings, prepared with ceramic materials like …

Modification of SS316 steel with the assistance of high velocity oxy fuel (HVOF) process to upsurge its sustainability

V Singh, A Bansal, AK Singla, DK Goyal… - Sustainable Materials …, 2023 - taylorfrancis.com
Vanadium carbide (VC) is an eminent hard material. However, the same has not been
sightsaw as an entrant coating material to provide sustainability for hydromachinery …

Testing of Polymer Composites for Manufacturing of Sprayer Nozzles

VE Slavkina, MA Mirzaev, AM Kuzmin, AI Kutyrev… - Polymers, 2024 - mdpi.com
Wear is the leading cause of nozzle failure. The durability of the nozzle is affected by the
material it is made from. Traditional materials are ceramics, stainless steel, brass, and …