S Sahu - US Patent 5,413,756, 1995 - Google Patents
US5413756A - Lead-free bearing bronze - Google Patents US5413756A - Lead-free bearing bronze - Google Patents Lead-free bearing bronze Download PDF Info Publication number …
GR Smith - US Patent 6,149,739, 2000 - Google Patents
An improved white manganese bronze alloy containing, in weight percent, about 1.0-3.0 wt% aluminum, about 2.0-4.0 wt% bismuth, about 53-59 wt% copper, about 0.8-2.0 wt% iron …
RL Greene, WJ Whitney, JM Carpenter - US Patent 6,854,183, 2005 - Google Patents
(57) ABSTRACT A lead-free bearing includes a bronze matrix powder metal bearing layer bonded to a Steelbacking a fully densified. The bearing material has about 8 to 12% by …
F Bin - US Patent 6,926,779, 2005 - Google Patents
A surface of aluminum alloy or iron alloy coated, on at least a part, with a lead-free copper- based coating layer comprising, by weight, 0.2–15% bismuth, and at least one metal …
WJ Griffin, R Ramamurthy, CE Cordy - US Patent 6,543,333, 2003 - Google Patents
A swashplate type compressor having a swashplate coated with a tin-cobalt alloy is provided. The alloy comprises between about 12 and 28 weight% cobalt, with the balance …
GR Smith - US Patent 8,097,208, 2012 - Google Patents
A white bronze alloy consisting essentially of, in weight percent, about 0.3-1.5 wt% aluminum, about 0.5-2.0 wt% bismuth, about 61-66 wt% copper, about 0.0-0.5 wt% iron …
S Sahu, AP Sahu - US Patent 8,449,697, 2013 - Google Patents
(57) ABSTRACT A silicon bearing, copper-nickel corrosion resistant and gall resistant alloy with the following weight percentage range is disclosed: Ni= 10-40; Fe= 1-10; Si= 0.5-2.5 …
D Venugopalan, S Sahu - US Patent 5,846,483, 1998 - Google Patents
US5846483A - Selenized dairy Se-Ni-Sn-Zn-Cu metal - Google Patents US5846483A - Selenized dairy Se-Ni-Sn-Zn-Cu metal - Google Patents Selenized dairy Se-Ni-Sn-Zn-Cu metal …