Deformation mechanism diagram and deformation instability of a Ti-5Al-5Mo-5V-1Cr-1Fe titanium alloy during the hot compression

Y Deng, Y An, Y Xiao, X Zhan, X Zhang… - Journal of Alloys and …, 2023 - Elsevier
Controlling the hot deformation mechanism of the titanium alloy and avoiding deformation
instability are the key points in the hot forging of the titanium alloy. A high throughput …

Novel insights on the near atomic scale spatial distributions of substitutional alloying and interstitial impurity elements in Ti-6Al-4V alloy

S Sahoo, O Licata, B Mazumder, S Roy - Journal of Alloys and Compounds, 2022 - Elsevier
The present study explores the near atomic scale spatial distributions of substitutional
alloying elements (aluminium and vanadium) and interstitial impurities (oxygen and carbon) …

Novel insights on the grain boundary α phase microstructure formation and orientation development in Ti-6Al-4V alloy

S Sahoo, S Roy - Journal of Alloys and Compounds, 2023 - Elsevier
The present work aims to understand the formation of microstructural features and their
orientation development at the (prior) β grain boundary regions for Ti-6Al-4V alloy. The grain …

Microstructure refinement and enhanced wear-resistance modulated by stress relaxation processing in a metastable β titanium alloy

K Hua, Y Zhang, F Zhang, H Kou, X Li, H Wu… - Materials …, 2021 - Elsevier
Hot deformation is an important procedure of metastable β titanium alloy for manufacturing.
And it is essential to improve the homogeneity of deformation microstructure in titanium …

[HTML][HTML] Transitions of deformation mechanisms in new metastable β-titanium Ti-1500G alloy

Y Ye, Y Han, S Zhang, J Le, F Chen, J Zhang, C Shen… - Materials & Design, 2025 - Elsevier
Ultrahigh-strength titanium alloy (≥ 1250 MPa) innovation calls for an integrated framework
combining novel deformation processing and microstructural control. However, a confluence …

Hydrogen Embrittlement Failure Behavior of Fatigue-Damaged Welded TC4 Alloy Joints

X Feng, Y Shi, W Zhang, K Volodymyr - Crystals, 2023 - mdpi.com
The interaction between fatigue damage and hydrogen in TC4 welded joints was analyzed
considering specimens with different pre-cycles. The fracture failure caused by hydrogen …

Micro-texture formation and the interrelation with bulk texture evolution in β deformation of Ti-6Al-4V alloy

S Sahoo, S Roy - Materials Characterization, 2025 - Elsevier
The present study explores the micro-texture formation based on the morphology and
orientation of the β grains, grain boundary (GB) α and lamellar or basketweave α phases …

Experimental and numerical investigation of the damage state of Ti-6Al-4V alloy sheet in the tensile test, hydraulic bulging, and hydroforming processes

YF Yapan, HG Korkmaz, S Toros, M Türköz - The International Journal of …, 2024 - Springer
There has not been any damage prediction using Johnson-Cook's (JC) hardening and
damage model in the hydraulic bulging (HB) and hydroforming (HF), which are the …

Microstructural characterization of improved formability of Ti-6Al-4V sheet by pulsating hydraulic bulging at room temperature

YF Yapan, O Öztürk, M Türköz, M Dilmeç… - Journal of Materials …, 2023 - Springer
This study aims to increase the limited formability of the Ti-6Al-4V sheet at room temperature
using the pulsating hydraulic bulging and to investigate the microstructural reasons for the …

High throughput construction for the deformation mechanism diagram and dynamic recrystallization of a bimodal‐sized particle‐reinforced Ti‐2.5 Zr‐2Al‐1 (Si, C) …

Y An, K Zhou, S Wei, S Zhu, Y Deng… - Materials Genome …, 2023 - Wiley Online Library
An in situ autogenous particle‐reinforced Ti‐2.5 Zr‐2Al‐1 (Si, C) titanium alloy is prepared