[HTML][HTML] Post-processing of additively manufactured metallic alloys–A review

A Malakizadi, D Mallipeddi, S Dadbakhsh… - International Journal of …, 2022 - Elsevier
Additive manufacturing (AM) is characterised by several unique advantages, such as
(freedom of) design, capability of fusing dissimilar materials, near-net-shape, and achieving …

Abrasive flow machining (AFM) finishing of conformal cooling channels created by selective laser melting (SLM)

S Han, F Salvatore, J Rech, J Bajolet - Precision Engineering, 2020 - Elsevier
Conformal cooling channels are widely adopted in the mold industry because of rapid and
uniform cooling during injection molding. These complicated cooling channel geometries …

Nontraditional finishing processes for internal surfaces and passages: a review

KL Tan, SH Yeo, CH Ong - Proceedings of the Institution of …, 2017 - journals.sagepub.com
The development of various nontraditional principles to finish the internal surfaces and
passages is reviewed. In particular, attention is focused on three relatively mature finishing …

[HTML][HTML] Post processing of additively manufactured 316L stainless steel by multi-jet polishing method

C Wang, YM Loh, CF Cheung, X Liang, Z Zhang… - Journal of Materials …, 2023 - Elsevier
Post-process finishing of the additively manufactured (AMed) surfaces is still a critical issue,
especially for the AMed surfaces with complex surface geometry, which largely limits the …

Surface finishing on IN625 additively manufactured surfaces by combined ultrasonic cavitation and abrasion

KL Tan, SH Yeo - Additive Manufacturing, 2020 - Elsevier
The poor and non-uniform surface quality of parts produced by powder bed fusion (PBF)
processes remains a huge limitation in additive manufacturing. Here we show that ultrasonic …

Synergistic effects in hydrodynamic cavitation abrasive finishing for internal surface-finish enhancement of additive-manufactured components

AP Nagalingam, HK Yuvaraj, SH Yeo - Additive Manufacturing, 2020 - Elsevier
Surface finishing additive-manufactured (AM) internal channels is challenging. In this study,
a novel hydrodynamic cavitation abrasive finishing (HCAF) technique is proposed and its …

Study on improvement of surface roughness and induced residual stress for additively manufactured metal parts by abrasive flow machining

C Peng, Y Fu, H Wei, S Li, X Wang, H Gao - Procedia Cirp, 2018 - Elsevier
Fabrication freedom is provided for production of metal parts with complex geometries that
cannot be fabricated by conventional subtractive manufacturing, as rapid advancements in …

Controlled hydrodynamic cavitation erosion with abrasive particles for internal surface modification of additive manufactured components

AP Nagalingam, SH Yeo - Wear, 2018 - Elsevier
The understanding and control of wear process can result in advances in manufacturing
science. For example, Surface finishing the internal surfaces of a component built using …

Experimental and numerical analyses of fluid flow inside additively manufactured and smoothed cooling channels

G Favero, G Berti, M Bonesso, D Morrone… - … Communications in Heat …, 2022 - Elsevier
The surface roughness can be considered one of the main drawbacks of the Laser Powder
Bed Fusion (LPBF) technology applied to thermal applications. Favero et al.[1] …

Abrasive flow machining applied to plastic gear matrix polishing

J Kenda, J Duhovnik, J Tavčar, J Kopač - The International Journal of …, 2014 - Springer
The topic of this paper is the application of abrasive flow machining (AFM) to gear tool
inserts polishing. Polished surface on plastic gear teeth improves surface geometry stability …