Axial fracture toughness of cold worked and stress relieved Zr-2.5 Nb pressure tube material containing deuterium between 5 and 200wppm was determined as per ASTM E− 1820-15 …
For the safety assessment of PHWR, it is required to study the flaw tolerance capacity of the pressure tubes as a function of the loading rate. In this work, the effect of loading rate and …
AK Bind, RN Singh… - Materials …, 2014 - asmedigitalcollection.asme.org
The need for improvement of the in-reactor performance of Zr-2.5% Nb pressure tubes arose because of the higher than expected diametral creep rates and variability in axial elongation …
The pressure tubes of Indian Pressurized Heavy Water Reactor (IPHWR) of 220 MWe are made of Zr–2.5 Nb alloy manufactured either from Double Melted (DM) or from Quadruple …
Previous work by one of the authors reported the stress-field for a fully-constrained hydride embedded in matrix computed using finite element method to develop an understanding of …
Fracture toughness and mechanical properties of the zircaloy-2 processed by rolling at different temperatures have been investigated, and simulations have been performed using …
The tensile and fracture behavior of ultrafine-grained Al 6061 alloy has been studied by experimental testing and extended finite element method simulation. The ultrafine-grained …
Abstract ASTM E1820-11, the most widely adopted standard for the determination of fracture toughness parameters, recommends two ductile crack growth correction methods for the …
The tensile properties and fracture toughness of Zr-2.5 Nb pressure tube materials manufactured for use in Indian PHWR220 and PHWR700 were evaluated. Tensile …