Impact of freeze–thaw cycles on low temperature mixed mode I/II cracking properties of water saturated hot mix asphalt: An experimental study

M Fakhri, SA Siyadati, MRM Aliha - Construction and Building Materials, 2020 - Elsevier
In cold regions, asphalt concrete cracking caused by low temperature is known as the most
important type of damage to asphaltic surfaces pavements. In rainy areas, the cold may …

The influence of natural and synthetic fibers on low temperature mixed mode I+ II fracture behavior of warm mix asphalt (WMA) materials

MRM Aliha, A Razmi, A Mansourian - Engineering Fracture Mechanics, 2017 - Elsevier
In this contribution, low temperature crack growth resistance of Warm Mix Asphalt (WMA)
mixtures reinforced with two types of fiber, namely natural Jute fiber and synthetic Polyolefin …

The effect of recycled PET bottles on the fracture toughness of polymer concrete

M Asdollah-Tabar, M Heidari-Rarani… - Composites …, 2021 - Elsevier
In this study, recycled polyethylene terephthalate (PET) bottles are shredded in different
sizes and added to the polymer concrete composition to investigate the effect on fracture …

Effects of cyclic freeze-thaw treatments on the fracture characteristics of sandstone under different fracture modes: laboratory testing

R Cao, C Wang, R Yao, T Hu, D Lei, H Lin… - Theoretical and Applied …, 2020 - Elsevier
For engineering projects in cold regions, the failure behaviour of jointed rocks is affected by
freeze–thaw (FT) cycle action. To reveal the fracture characteristics of rock under the …

Study of characteristic specification on mixed mode fracture toughness of asphalt mixtures

MRM Aliha, H Behbahani, H Fazaeli… - Construction and Building …, 2014 - Elsevier
Low temperature cracking is one of the main deterioration and failure modes for pavements.
Hence, in this paper the effect of asphalt characteristic on its mixed mode I/II low temperature …

Influence of specimen geometry on mode I fracture toughness of asphalt concrete

S Fuan, M Ke, L Kanghe, L Kun, MRM Aliha - Construction and Building …, 2021 - Elsevier
Determination of fracture toughness (K Ic) for the asphalt mixture concrete requires
employment of suitable testing methods and specimens. Disc-shape specimens are among …

Effect of temperature and air void on mixed mode fracture toughness of modified asphalt mixtures

MRM Aliha, H Fazaeli, S Aghajani, FM Nejad - Construction and Building …, 2015 - Elsevier
The use of modified asphalt mixtures is a suitable solution for preventing low temperature
cracking of pavements in cold regions. In this paper, mixed mode I/II fracture toughness of …

[HTML][HTML] Comparison of testing method effects on cracking resistance of asphalt concrete mixtures

D Yang, HR Karimi, MRM Aliha - Applied Sciences, 2021 - mdpi.com
As an inherent characteristic of materials, the fracture toughness is an important parameter
to study the cracking behavior of asphalt concrete mixtures. Although material compositions …

Fracture toughness determination of modified HMA mixtures with two novel disc shape configurations

MRM Aliha, MJ Sarbijan, A Bahmani - Construction and Building Materials, 2017 - Elsevier
In this paper two circular shape test specimens are designed and examined for experimental
determination of mode I fracture toughness (K Ic) in different modified hot mix asphalt (HMA) …

Evaluation of fracture resistance of asphalt concrete involving Calcium Lignosulfonate and Polyester fiber under freeze–thaw damage

M Zarei, AA Kordani, M Khanjari, M Zahedi - Theoretical and Applied …, 2022 - Elsevier