Progress in metal corrosion mechanism and protective coating technology for interconnect and metal support of solid oxide cells

J Mao, E Wang, H Wang, M Ouyang, Y Chen… - … and Sustainable Energy …, 2023 - Elsevier
Solid oxide cell (SOC) is an important technology for hydrogen energy utilization. Durability
and reliability of metal components including interconnect and metal support of metal …

[HTML][HTML] Long-term (4 year) degradation behavior of coated stainless steel 441 used for solid oxide fuel cell interconnect applications

C Goebel, R Berger, C Bernuy-Lopez… - Journal of Power …, 2020 - Elsevier
The present work aims to investigate the long-term stability of Ce/Co coated AISI 441 used
as an interconnect material in solid oxide fuel cells (SOFC). Being a commercially available …

Atomic spectrometry update. Review of advances in the analysis of metals, chemicals and functional materials

B Gibson, S Carter, AS Fisher, S Lancaster… - Journal of Analytical …, 2014 - pubs.rsc.org
This review covers developments in the analysis of chemicals, metals and functional
materials. We have strengthened the criticality of this review and have included only those …

Corrosion behaviour of AISI 430 stainless steel in O2-40% H2O at 800° C

P Wiman, T Thublaor, T Rojhirunsakool… - Corrosion …, 2022 - Elsevier
Less mass gain and poorer scale adhesion assessed by the tensile test of the AISI 430
stainless steel exposed to O 2-40% H 2 O at 800° C were observed in comparison with the …

High temperature oxidation behaviour of Fe–15.7 wt.% Cr–8.5 wt.% Mn in oxygen without and with water vapour at 700 ºC

S Chandra-Ambhorn, P Saranyachot, T Thublaor - Corrosion Science, 2019 - Elsevier
Abstract Fe–15.7 wt.% Cr–8.5 wt.% Mn was oxidised in O 2 and O 2–9 vol.% H 2 O at 700°
C. Oxide scales in both atmospheres consisted of M 2 O 3 and M 3 O 4 where M could be …

Effect of water vapor on high-temperature oxidation of NiAl alloy

D Zhu, X Wang, J Zhao, J Lu, Y Zhou, C Cai, J Huang… - Corrosion …, 2020 - Elsevier
The high-temperature oxidation of NiAl is studied with dry oxygen and water vapor. The
oxidation in H 2 O results in a thicker Al 2 O 3 oxide scale than that in O 2. The oxide scale …

Component analysis of a 25-cell stack following 6.7 kh of high temperature electrolysis

J Aicart, K Couturier, M Hubert, K Vulliez, M Elie… - International Journal of …, 2024 - Elsevier
The demonstration of relevant lifetimes for solid oxide electrolysis stacks is an underlying
necessity to the rapidly industrializing technology. Following a 6.7 kh test of a 25-cell stack …

Impact of pre-oxidation on the reactivity and conductivity in H2–H2O atmosphere of a ferritic stainless steel for high temperature water vapour electrolysis

MR Ardigo-Besnard, I Popa, S Chevalier - International Journal of …, 2022 - Elsevier
The as-rolled K41X (AISI 441) ferritic stainless steel presents unusual behaviour when
exposed in H 2–H 2 O atmosphere at 800° C, with growth of non-protective iron oxides at its …

Precipitation of metallic Ni clusters in alumina scale during high-temperature oxidation of NiAl in water vapor

D Zhu, J Chen, J Chen, X Zhang, H Sun, X Wang… - Corrosion …, 2024 - Elsevier
Water vapor is ubiquitously present for energy conversion and combustion systems, yet its
effect on the oxidation of crucial structure components of heat-resistant alloys remains …

Effect of deposition temperature on corrosion behavior of CVD aluminide coatings on K452 superalloy

J Xu, S Geng, J Wang, G Chen, F Wang, Q Sun… - Surface and Coatings …, 2025 - Elsevier
Aluminide coatings are deposited on K452 alloy by chemical vapor deposition (CVD)
method at 850, 950 and 1050° C, respectively. All coatings consist of a β-NiAl layer and an …