A major goal in printing soft magnetic Fe-Si steels using additive manufacturing is to take advantage of the potential for complex geometric designs and site-specific grain control …
Annealing of laser powder bed fusion (LPBF) processed Fe-49Co-2 V (Hiperco) samples at 865° C for 4 h leads to a substantial improvement in its soft magnetic properties. While the …
A widespread implementation of large scale additive manufacturing (AM) processes, such as wire arc-directed energy deposition (WA-DED) AM can transform the current …
Thin-walled structures are being used in soft magnetic components manufactured by additive manufacturing to limit eddy current losses in AC machines. Fe-6.5 wt% Si has been …
Annealing of laser powder bed fusion (LPBF) processed Fe-49Co-2 V (Hiperco) samples at 865◦ C for 4 h leads to a substantial improvement in its soft magnetic properties. While the as …