Dry sliding wear behaviour of in situ Al–TiB2 composites

K Niranjan, PR Lakshminarayanan - Materials & Design, 2013 - Elsevier
Aluminium matrix/titanium diboride reinforced (Al/TiB2) composites were fabricated by in situ
process. The wear behaviour was studied by using a pin-on-disc wear tester at room …

Developing partially oxidized NiCr coatings using the combined flame spray and plasma spray process for improved wear behaviour at high temperature

SR Medabalimi, MR Ramesh, R Kadoli - Wear, 2021 - Elsevier
The powders of NiCrBSiFe and NiCr are partially oxidized using a flame spray process and
are deposited on MDN321 steel substrate using a plasma spray process. The effect of partial …

Effect of sintering parameters on densification, corrosion and wear behaviour of Ni-50Fe alloy prepared by spark plasma sintering

MI Makena, MB Shongwe, MM Ramakokovhu… - Journal of Alloys and …, 2017 - Elsevier
Spark plasma sintering (SPS) technique was used to fabricate Ni50Fe alloys. Powders were
sintered at various temperatures, pressure and holding times ranging between 900 and …

Microstructural charactistics of plasma sprayed NiCrBSi coatings and their wear and corrosion behaviors

S Huang, J Zhou, K Sun, H Yang, W Cai, Y Liu, P Zhou… - Coatings, 2021 - mdpi.com
Nickel-based alloys are commonly used as protective coating materials for surface
protection applications owing to their superior resistance to corrosion, wear and high …

Differentiation of specific wear rates of AISI 304 austenitic and AISI 2205 duplex stainless steels at room and high temperatures

DA Ahmed, MM Mulapeer - Heliyon, 2022 - cell.com
Austenitic and duplex stainless steels are used in numerous applications at room and high
temperatures. However, their wear behaviour at high temperatures has not yet been …

Effect of strain hardening on wear and corrosion resistance of 316L Austenitic stainless steel

G Sun, J Huang, J Peng, W Wu - Journal of Materials Engineering and …, 2024 - Springer
The wear and corrosion resistance of 316L austenitic stainless steel after strain hardening
were studied. 316L austenitic stainless steel was composed of a large amount of austenite …

Thermal spray coatings for blast furnace tuyere application

A Pathak, G Sivakumar, D Prusty, J Shalini… - Journal of Thermal …, 2015 - Springer
The components in an integrated steel plant are invariably exposed to harsh working
environments involving exposure to high temperatures, corrosive gases, and erosion/wear …

[PDF][PDF] Comparison of specific wear rates of austenitic and super austenitic stainless steels at high temperatures

D Ahmed, M Mulapeer - Zanco Journal of Pure and Applied Sciences, 2022 - iasj.net
Due to the relatively high wear rate of the austenitic stainless steel S30400 and the high
mechanical properties of the super austenitic stainless steel S31254, it was possible to …

Effect of argon gas environment on high temperature sliding wear characteristics of NiCrBSi laser clad

AK Jaiswal, AR Govande, KUV Kiran, BR Sunil… - Materials Today …, 2023 - Elsevier
The martensitic stainless steels find extensive application in steam turbine blades, marine
turbine blades, compressor blades etc. due to the optimum combination of strength and …

Densification behaviour and the effect of heat treatment on microstructure, and mechanical properties of sintered nickel-based alloys

N Kekana, MB Shongwe, OT Johnson… - The International Journal …, 2019 - Springer
The present work focused on the densification behaviour and heat treatment effect on the
mechanical properties of spark plasma sintered Ni–Fe–Al–Cr alloys. Five initial alloys were …