[HTML][HTML] Irradiation-induced clustering in a high-Ni, high-Mn, low-Cu boiling water reactor pressure vessel weld after 28 full power years

D Mayweg, K Lindgren, P Efsing, M Thuvander - Scripta Materialia, 2025 - Elsevier
Abstract High-Ni, high-Mn welds are the life-time determining components in reactor
pressure vessels (RPVs) of Nordic reactors at desired operating times of pressurized water …