High temperature oxidation behavior of a novel Ni-Cr-W-Al-Ti superalloy

J Teng, X Gong, B Yang, S Yu, R Lai, J Liu, Y Li - Corrosion Science, 2022 - Elsevier
Oxidation of a novel Ni-19Cr-17W-2Al-0.5 Ti superalloy was investigated in air at 800–1100°
C. In spite of the local spallation of external oxide scale after prolonged oxidation at high …

Formation and evolution behavior of M6C carbide in a Ni-W-Cr superalloy

M Huang, Z Zhou, C Cui, R Zhang, Z Shi, X Wang… - Materials …, 2023 - Elsevier
The carbide formation and evolution of a new Ni-26W-6Cr (wt.%) superalloy for the 800° C
molten salt reactor (MSR) was investigated by homogenization heat treatment tests and the …

Influence of Ti addition on oxidation behavior of Ni-Cr-W-based superalloys

J Teng, X Gong, B Yang, S Yu, J Liu, Y Li - Corrosion Science, 2021 - Elsevier
Abstract Effect of Ti addition on oxidation behavior of Ni-Cr-W alloys was systematically
investigated by isothermal oxidation in air. The oxidation rate is accelerated by Ti addition …

Corrosion of Incoloy 800H alloys with nickel cladding in FLiNaK salts at 850 C

Q Dai, XX Ye, H Ai, S Chen, L Jiang, J Liang, K Yu… - Corrosion …, 2018 - Elsevier
The corrosion of 800H alloy with and without Ni-cladding, as well as GH3535 alloy, in
molten FLiNaK salts at 850° C has been investigated. Results show that Cr and Fe are …

On the possibility of severe corrosion of a Ni-W-Cr alloy in fluoride molten salts at high temperature

H Ai, XX Ye, L Jiang, B Leng, M Shen, Z Li, Y Jia… - Corrosion …, 2019 - Elsevier
The corrosion of a Ni-26W-6Cr alloy, as well as GH3535 alloy, in the FLiNaK salts at 800° C
was investigated by static immersion corrosion, combining with the electrochemical …

Revealing 3D morphological and chemical evolution mechanisms of metals in molten salt by multimodal microscopy

A Ronne, L He, D Dolzhnikov, Y Xie, M Ge… - … applied materials & …, 2020 - ACS Publications
Growing interest in molten salts as effective high-temperature heat-transfer fluids for
sustainable energy systems drives a critical need to fundamentally understand the …

Effect of Zr addition on the microstructure and intermediate-temperature mechanical performance of a Ni–26W–6Cr based superalloy

S Liu, XX Ye, L Jiang, R Liu, Z Gao, X Gong, Z Li… - Materials Science and …, 2022 - Elsevier
In the present work, Zr was added into a Ni–26W–6Cr alloy to improve the intermediate
temperature ductility, and the corresponding mechanism was discussed. The enrichment of …

Optimized spacing of active sites in Ni-Mo catalysts enhances ethanol production in syngas conversion

Y Ren, Y Weng, S Meng, C Huang, Q Sun… - Applied Catalysis B …, 2025 - Elsevier
The direct conversion of syngas to ethanol is highly attractive but remains challenging due to
low CO conversion and poor EtOH/ROH. We investigated the conversion of syngas over a …

Metallic impurities induced corrosion of a Ni-26W-6Cr alloy in molten fluoride salts at 850 oC

H Ai, S Liu, XX Ye, L Jiang, B Zhou, X Yang, B Leng… - Corrosion …, 2021 - Elsevier
The effect of metallic impurities on corrosion of a Ni-26W-6Cr alloy in molten FLiNaK salts at
850° C was investigated. Results show that the Ni-26W-6Cr alloy exhibits the same …

Welding solidification cracking susceptibility and behavior of a Ni-28W-6Cr alloy

S Chen, XX Ye, DKL Tsang, L Jiang, K Yu, C Li… - Journal of Materials …, 2019 - Elsevier
Welding solidification cracking of alloys is associated with the range of solidification